Nano-treating is a novel concept wherein a low percentage of nanoparticles is used for microstructural control and property tuning in metals and alloys. The nano-treating of AA7075 was investigated to control its microstructure and improve its structural stability for high performance. After treatment with TiC nanoparticles, the grains were significantly refined from coarse dendrites of hundreds of micrometers to fine equiaxial ones smaller than 20 μm. After T6 heat treatment, the grains, with an average size of 18.5 μm, remained almost unchanged, demonstrating an excellent thermal stability. It was found that besides of growth restriction factor by pinning behavior on grain boundries, TiC nanoparticles served as both an effective nucleation agent for primary grains and an effective secondary phase modifier in AA7075. Furthermore, the mechanical properties of nano-treated AA7075 were improved over those of the pure alloy. Thus, nano-treating provides a new method to enhance the performance of aluminum alloys for numerous applications.
Invar is a solid solution alloy that offers high-dimensional stability. It is challenging for traditional methods to strengthen Invar alloys without a significant increase in the coefficient of thermal expansion (CTE). In this work, WC nanoparticle-reinforced Invar nanocomposite was manufactured. The microstructures, mechanical properties, and thermal expansion behavior were investigated. It was found that the Invar alloy was effectively strengthened by WC nanoparticle reinforcement without significant elevation of its CTE. The Invar–WC nanocomposite exhibits an enhanced yield and tensile strength of 440 and 795 MPa, an increase of 60% and 77% from commercial Invar alloy, and a moderate ductility of 22.7% in annealed state. In cold-rolled state, The Invar–WC nanocomposite exhibits a high tensile strength of 1050 MPa, an increase of 46% from commercial Invar alloy, while retaining 4.5% ductility. A record low CTE value of 2.61 × 10−6/°C and an enhanced Young’s modulus of 185 GPa, up from 140 GPa, were also achieved. It was found that WC leads to a lower CTE at higher temperature compared to unreinforced Invar.