A key hallmark of atomic layer deposition (ALD) is that it proceeds via self-limiting reactions. For a good ALD process, long reactant exposure times beyond that required for saturation on planar substrates can be useful, for example, to achieve conformal growth on high aspect ratio nanoscale trenches, while maintaining consistent deposition across large-area surfaces. Area-selective deposition (ASD) is becoming an enabling process for nanoscale pattern modification on advanced nanoelectronic devices. Herein, we demonstrate that during area-selective ALD, achieved by direct coupling of ALD and thermal atomic layer etching (ALE), excess reactant exposure can have a substantially detrimental influence on the extent of selectivity. As an example system, we study ASD of TiO2 on hydroxylated SiO2 (Si–OH) vs hydrogen-terminated (100) Si (Si–H) using TiCl4/H2O for ALD and WF6/BCl3 for ALE. Using in situ spectroscopic ellipsometry and ex situ x-ray photoelectron spectroscopy, we show that unwanted nucleation can be minimized by limiting the water exposure during the ALD steps. Longer exposures markedly increased the rate of nucleation and growth on the desired non-growth region, thereby degrading selectivity. Specifically, transmission electron microscopy analysis demonstrated that near-saturated H2O doses enabled 32.7 nm thick TiO2 patterns at selectivity threshold S > 0.9 on patterned Si/SiO2 substrates. The correlation between selectivity and reactant exposure serves to increase fundamental insights into the effects of sub-saturated self-limiting surface reactions on the quality and effectiveness of ASD processes and methods.
Atomic layer deposition (ALD) has been a promising technique in fabricating membranes and tuning their properties with a precision at the atomic level. Fabrication of zeolitic imidazolate framework (ZIF) membranes using the ligand‐induced permselectivation (LIPS) method starts with the formation of an oxide in a mesoporous substrate by ALD and is followed by the transformation of this oxide to ZIF using imidazolate vapor treatment. The objective of the ALD step is to block the mesopores with a thin deposit, that is, one with small penetration depth and small thickness on the top surface of the substrate. Unlike typical ALD on nonporous substrates, where all available sites react per ALD cycle, thin deposit formation in a mesoporous substrate requires that only a small fraction of the available deposition sites (i.e., close to the substrate surface) is subjected to ALD. Consequently, reactant dosing and duration of pulses are important process variables which, together with diffusion and reaction kinetics determine the deposit structure. Quantitative understanding of the interplay of these variables and phenomena can enable the rational design of ALD within mesoporous substrates. Here, we extend our earlier modeling effort considering the coexistence of ALD both inside the pores and on the external surface of the substrate. Finite‐volume based models were developed and validated to simulate the two distinct modes of deposition cycle by cycle. The total mass uptake of the substrate with ALD cycles can be predicted using the combined surface deposition and pore reaction–diffusion models as affirmed by in situ quartz crystal microbalance experimental data. The ALD reactor model combined with the deposition model can accurately capture the number of ALD cycles needed to block the pores of the substrate. Based on the model, we designed a modified ALD process and examined the performance of the corresponding LIPS membranes. The present modeling work provides a new understanding of the deposit formation via ALD within mesoporous substrates for a variety of membrane applications.
Bottom-up self-aligned area-selective deposition (ASD) plays an important role in patterning of advanced electronic devices. Specifically, ASD of organic materials can be utilized for nucleation inhibitors, sacrificial layers, and air-gap materials for next-generation nanoscale processing. This work introduces fundamental growth behavior of various conjugated polymers including polypyrrole, polythiophene, and polyaniline via oxidative molecular layer deposition and chemical vapor deposition. Effects of process parameters on film properties are described, and ASD behavior of different polymers are quantitatively characterized. These findings expand fundamental understanding of conjugated polymer deposition and provide new perspectives for ASD of organic thin films.