Ferroelectric (Hf,Zr)O2 thin films have attracted increased interest from the ferroelectrics community and the semiconductor industry due to their ability to exhibit ferroelectricity at nanoscale dimensions. The properties and performance of the ferroelectric (Hf,Zr)O2 films generally depend on various factors such as surface energy (e.g., through grain size or thickness), defects (e.g., through dopants, oxygen vacancies, or impurities), electrodes, interface quality, and preferred crystallographic orientation (also known as crystallographic texture or simply texture) of grains and/or domains. Although some factors affecting properties and performance have been studied extensively, the effects of texture on the material properties are still not understood. Here, the influence of texture of the bottom electrode and Hf0.5Zr0.5O2 (HZO) films on properties and performance is reported. The uniqueness of this work is the use of a consistent deposition process known as Sequential, No-Atmosphere Processing (SNAP) that produces films with different preferred orientations yet minimal other differences. The results shown in this study provide both new insight on the importance of the bottom electrode texture and new fundamental processing-structure–property relationships for the HZO films.
A key hallmark of atomic layer deposition (ALD) is that it proceeds via self-limiting reactions. For a good ALD process, long reactant exposure times beyond that required for saturation on planar substrates can be useful, for example, to achieve conformal growth on high aspect ratio nanoscale trenches, while maintaining consistent deposition across large-area surfaces. Area-selective deposition (ASD) is becoming an enabling process for nanoscale pattern modification on advanced nanoelectronic devices. Herein, we demonstrate that during area-selective ALD, achieved by direct coupling of ALD and thermal atomic layer etching (ALE), excess reactant exposure can have a substantially detrimental influence on the extent of selectivity. As an example system, we study ASD of TiO2 on hydroxylated SiO2 (Si–OH) vs hydrogen-terminated (100) Si (Si–H) using TiCl4/H2O for ALD and WF6/BCl3 for ALE. Using in situ spectroscopic ellipsometry and ex situ x-ray photoelectron spectroscopy, we show that unwanted nucleation can be minimized by limiting the water exposure during the ALD steps. Longer exposures markedly increased the rate of nucleation and growth on the desired non-growth region, thereby degrading selectivity. Specifically, transmission electron microscopy analysis demonstrated that near-saturated H2O doses enabled 32.7 nm thick TiO2 patterns at selectivity threshold S > 0.9 on patterned Si/SiO2 substrates. The correlation between selectivity and reactant exposure serves to increase fundamental insights into the effects of sub-saturated self-limiting surface reactions on the quality and effectiveness of ASD processes and methods.
During TiO2 atomic layer deposition (ALD) using TiCl4 and H2O at ∼150 °C, nucleation proceeds rapidly on hydroxylated SiO2 but is inherently delayed on passivated surfaces such as H-terminated silicon (Si-H) and trimethylsilyl-passivated SiO2 (SiO2-TMS) formed using dimethylamino-trimethylsilane (DMA-TMS) as a small molecule inhibitor. In this work, we explore details of TiO2 nucleation on both Si-H and SiO2-TMS and show that the mechanisms leading to unwanted nuclei depend strongly on the passivation mechanism. Initial growth is observed as a function of ALD cycles using scanning electron microscopy to obtain average particle size, density, and overall surface coverage fraction. Also, average film thickness vs cycle is estimated using ellipsometry or Rutherford backscattering spectrometry. Data are compared to an analytical model that considers that either nucleation sites are present on the starting non-growth surface or sites are generated during the ALD process. On the Si-H surface, data and modeling indicate that nucleation occurs predominantly from a fixed number of nucleation sites present on the starting growth surface that start to immediately grow. However, on TMS-passivated SiO2, nucleation sites are predominantly generated during the growth process so that the density of nucleation sites increases as growth proceeds. Results indicate that nucleation sites are created when adsorbed ALD reactants become kinetically trapped on the SiO2-TMS surface. This demonstrates that mechanisms associated with unwanted nucleation during area-selective deposition (ASD) can depend on details of the surface passivation scheme, thereby providing insight to help to improve ASD strategies for advanced applications.