27 January 2025 in Corrosion Science
Verified
Journal Article
Open access
TBTatiana Blank
Tatiana Blank
SBSabine Behrens
Sabine Behrens
ELElisabeth Franziska Lange
Elisabeth Franziska Lange
CKChristian Klose
Christian Klose
DCDemircan Canadinc
Demircan Canadinc
HMHans Maier
Hans Maier

6 March 2026 in Electrochimica Acta
Verified
Journal Article
Closed access
AHAzizeh Hosseinjany
Azizeh Hosseinjany
TBTatiana Blank
Tatiana Blank
DCDemircan Canadinc
Demircan Canadinc
MYM. Baris Yagci
M. Baris Yagci
HMHans Maier
Hans Maier

9 July 2024 in PLOS ONE
Verified
Journal Article
Open access
PDF file
TBTatiana Blank
Tatiana Blank
AAAndré Marcel Ahrens
André Marcel Ahrens
CKChristian Klose
Christian Klose
DCDemircan Canadinç
Demircan Canadinç
TLThomas Lenarz
Thomas Lenarz
HMHans Maier
Hans Maier
Platinum and platinum-based alloys are used as the electrode material in cochlear implants because of the biocompatibility and the favorable electrochemical properties. Still, these implants can fail over time. The present study was conducted to shed light on the effects of microstructure on the electrochemical degradation of platinum. After three days of stimulation with a square wave signal, corrosive attack appeared on the platinum surface. The influence of mechanical deformation, in particular rolling, on the corrosion resistance of platinum was also prominent. The cyclic voltammetry showed a clear dependence on the electrolyte used, which was interpreted as an influence of the buffer in the artificial perilymph used. In addition, the polarization curves showed a shift with grain size that was not expected. This could be attributed to the defects present on the surface. These findings are crucial for the manufacture of cochlear implants to ensure their long-term functionality.

12 October 2026 in Materials Chemistry and Physics
Verified
Journal Article
Open access
TBT. Blank
T. Blank
NEN. Ehlert
N. Ehlert
MGM.K. Goerlich
M.K. Goerlich
CKC. Klose
C. Klose
TLT. Lenarz
T. Lenarz
HMHans Maier
Hans Maier

1 December 2024 in Advanced Engineering Materials
Verified
Journal Article
Open access
EBElmar Jonas Breitbach
Elmar Jonas Breitbach
SJStefan Julmi
Stefan Julmi
SBSabine Behrens
Sabine Behrens
TBTatiana Blank
Tatiana Blank
AAArvid Abel
Arvid Abel
HMHans Maier
Hans Maier
Magnesium alloys pose challenges in additive manufacturing, due to the difference between the melting temperature of magnesium oxide (2825 °C) on the powder particles and the boiling point of metallic magnesium (1093 °C). A promising approach to overcoming the difficulties is the reduction of the thickness of the high‐melting oxide layer on the surface of the particles. Magnesium alloys, each containing varying amounts of strontium, neodymium, and yttrium, are cast and subsequently analyzed in terms of their microstructures, mechanical properties, oxide layer thicknesses, and corrosion behavior. Alloying magnesium with strontium results in a reduction of the oxide layer thickness, which reaches a minimum of 0.5 wt% strontium content. The presence of rare earth elements increases the strength of the alloys, although the inclusion of neodymium results in an increase in the oxide layer thicknesses. On the other hand, the oxide layer thickness remains unaffected when alloying with yttrium. However, further increases in strontium content up to the monolithic phase Mg17Sr2 have been found to result in a reduced effect on the open‐circuit potential. Further studies should be conducted to investigate the suitability of strontium as an alloying element to reduce the oxide layer thickness of magnesium particles.