15 July 2023 in ISIJ International
In the industrial steel manufacturing process, such as continuous casting and ingot casting, macrosegregation occurs due to the effect of bridging and contraction flow during the middle and end periods of solidification. Since the macrosegregation results in a nonuniform structure and eventually cracks, there has been a demand for technological development that does not cause macrosegregation in the casting process. In this study, model experiments using the medium-carbon steel cast with a laboratory-scale local-chilled mold at different superheating have been carried out to investigate the relationship between solidified structure and macrosegregation occurred by local bridging during casting. The morphology of shrinkage porosities and dendrite structures was observed. The concentrations of the alloying elements were analyzed for macrosegregation by an electron probe micro-analyzer. Chill plates successfully formed the columnar dendrite bridging area and the columnar dendrite shell in the sample with high superheating. During solidification, the negative pressure of the region below the bridging increased, and the concentrated contraction flow flowed into the bottom of the large shrinkage porosity. Finally, V segregation was formed in the bridging area, large shrinkage porosities remained below the bridging area, and point-like or band-like positive macrosegregation occurred in the interdendritic region between columnar dendrites and equiaxed dendrites below the bridging. In comparison, a lower casting temperature increased the grain density and formed shrinkage porosities that were smaller in size but larger in number and more dispersed.
15 July 2023 in ISIJ International
Currently, steel products are manufactured by continuous casting or large-sized ingot casting, and macrosegregation that occurs during the manufacturing process significantly impacts product quality in terms of cracks and deterioration of mechanical properties. To clarify the principle of casting defects, such as shrinkage porosity and macrosegregation due to the formation of bridging of the columnar dendrite of the medium-carbon steel, in this experiment, a laboratory-scale local-chilled mold in which the middle part was forcedly cooled was designed to cause bridging, shrinkage porosities, and macrosegregation. Enough risers were also designed to simulate realistic gravity casting as much as possible. The solidification structure morphology was observed, concentration analysis of alloying elements was performed, and the effect of bridging on macrosegregation was investigated. Solidification proceeded preferentially from the chill plate, and the bridging was formed successfully at a high casting temperature. The high casting temperature condition could cause bridging, but large shrinkage porosities would be formed as well. On the contrary, the lower casting temperature condition could increase the grain density and form shrinkage porosities that are smaller in size but larger in number and more dispersed, compared with the case cast with no chill plate mold. Due to the formation of bridging, macrosegregation was formed, and the difference between positive and negative segregation was increased from the longitudinal center of the sample.