Because of its hardness, wear-resistance, strength, and bending capabilities, beech wood is a widely-used hardwood in Europe. It is mainly used for furniture, floors, construction, veneer boards, and laminated wood. For such uses, the mechanical properties are very important, especially in cases of impact loads. The aim of this work is to analyse the mechanical properties of beech wood samples exposed to compressive force in the longitudinal direction based on different loading rates (in the range from 10 mm/min to 500 mm/min). Stress–strain diagrams were made with the experimental data, and mathematical functions were fit to them. Using the fit functions, the following properties of beech wood samples were determined: the stress and strain at the elastic limit; the maximum stress and associated strain; the modulus of elasticity; the tangent modulus; the specific energy of elastic strain; and the specific energy of plastic strain. The results showed that by increasing the loading rates, the elastic properties of beech wood increase, while the analysed plastic properties do not show a clear tendency of changes with increase of the loading rates.
17 January 2023 in Wood Material Science & Engineering
The article presents an analysis of the influence of simulated circular saw teeth marks profile in relation to the anatomical roughness of solid oak wood (Quercus robur L.) on machining roughness after sawing along the grain with a circular saw in order to better understand this relationship and to improve the knowledge how this two factors can be separated for further analysis in real-world sawing and to try to quantify the minimum theoretical tooth mark height that could be distinguished from anatomical roughness of wood. The signal-to-noise ratio (SNR) of simulated circular saw teeth mark signal in relation to measured anatomical roughness signal of solid oak wood was used to determine the level at which saw teeth marks could have a meaningful impact on machined surface roughness. From the analysis it can be concluded that SNR values even as low as −13 dB can have enough information to be used for frequency analysis and filtering out of tooth marks signal. Averaging and longer sampling lengths provide much better SNR values and provide the frequency spectrum of the structural roughness signal of solid oak wood with the highest amplitude of less than 0.5 μm. If more favorable SNR values are to be obtained, sampling lengths should be much longer than what is standardly used and recommended in ISO 3274: 1996 (in this research cumulative sampling length of 600 mm was used).
The article presents the method for an objective determination of threshold value, needed for filtering out the anatomical roughness signal, with filter based on fast Fourier Transform (FFT), from surface roughness profile after machining. The method...