8 May 2019 in Journal of Testing and Evaluation
The development of the multiple stress creep and recovery (MSCR) test represented an improvement in the evaluation of the rutting susceptibility of asphalt binders. However, the creep and recovery times of the current test protocol (1 and 9 s, respectively) may not be adequate to predict performance under extremely heavy and slow traffic conditions or to allow full recovery of polymer-modified binders. Highly modified asphalt binders have been increasingly used in pavements under severe traffic and weather conditions, and, because of the higher polymer content in these materials, they can be more sensitive to variations in loading times and stresses. However, the influence of different loading times has not been investigated in detail for these materials yet. In this article, the effect of longer creep and recovery times on the MSCR test was evaluated for a highly modified asphalt binder, and the results were compared with those obtained for a neat asphalt binder and a regular styrene-butadiene-styrene (SBS) modified binder. Tests were carried out at the high performance grading temperature of each binder. and three situations were analyzed: (i) the increase of creep time to 2, 4, and 8 s; (ii) the increase of recovery time to 240 and 500 s; and (iii) the increase of both times simultaneously, to 2/18 s and 3/27 s. The highly modified binder analyzed was more susceptible to variation in creep and recovery times than the other binders and showed considerable increase in compliance due to nonlinear behavior, although there is no evidence that this was caused by the high polymer amount in this material. The results support the need of further investigation in this subject for future refinements in the MSCR test protocol and the specification criteria for slow or standing traffic, so that the susceptibility to longer loading times can be properly considered.
1 March 2020 in Journal of Transportation Engineering, Part B: Pavements
The large-stone asphalt mixture is a promising approach to improve rutting resistance of roads under very heavy traffic. This paper describes the rehabilitation of two test sections in Brazil using a composite of dense graded asphalt mixtures with typical (9.5 or 19 mm) and large-stone (32 mm) nominal maximum aggregate size to decrease rutting while simultaneously preserving the functional surface qualities of the pavement. The asphalt mixtures used in this study were characterized for their linear viscoelastic properties using dynamic modulus and rutting resistance using the French wheel tracking test. The rehabilitated pavement was monitored over a period of 2 years and demonstrated minimal rutting. This was in contrast to the 12–15 mm rutting that occurred over just 1 year prior to the rehabilitation when only 9.5- and 12.5-mm size dense graded mixture was used on the surface with different asphalt binders. This study also demonstrates that this difference in field performance was not reflected when using viscoelastic layered analysis of the pavement structure, which is a recognized limitation when damage analysis is not considered.
15 May 2020 in Transportes
It is still a challenge to produce recycled asphalt mixtures with increased contents of reclaimed asphalt pavement (RAP) without compromising field performance. On hot and warm recycling, the RAP binder is activated, but the amount that truly interacts with the fresh binder is unknown. The present study describes the application of a staged extraction laboratory procedure to evaluate the homogeneity of the binder film in two plant-produced warm mixtures, one containing 25% RAP and the other without RAP (control mixture). The “layers” of binder obtained through the procedure were tested in the Dynamic Shear Rheometer. Results showed a progressive variation of the parameters for the 25% RAP mixture, which was not observed for the control mixture. The procedure was useful to determine binder homogeneity in recycled mixtures, which can be related to the degree of blending between RAP and fresh binders, providing useful information to ensure adequate field performance.
1 January 2017 in Transportation Research Record: Journal of the Transportation Research Board
Reflective cracking is a common issue with respect to rehabilitated asphalt pavements, especially when the rehabilitation is done by applying a hot-mix asphalt overlay on the existing damaged pavement. Several approaches can be adopted to delay reflective cracking. They include an increase of the overlay thickness and the use of a stress relief asphalt mixture (SRAM), which is a fine-graded, flexible, and thin asphalt interlayer. Because the efficiency of a SRAM is highly related to the properties of the asphalt binder used in the mixture, it is of interest to use a highly modified asphalt (HiMA) binder. This paper describes a field test comprising three sections at BR-116 (a heavily trafficked highway in Brazil). One of the rehabilitation strategies used for a cracked asphalt pavement was a 2.5-cm SRAM (produced with a HiMA binder) and 5-cm styrene–butadiene–styrene (SBS) hot-mix asphalt (HMA). The other two strategies were to apply SBS HMA overlays of different thicknesses (7.5 cm and 10.5 cm). The aim was to evaluate and compare the capability of these solutions to control reflective cracking. Rheological properties and multiple stress creep and recovery tests were performed on the asphalt binders, and the semicircular bending test was performed on the asphalt mixtures. The surface conditions were monitored, and the results for each section were compared. After a 29-month period, the section that received the interlayer had the lowest cracked area and showed better resistance than the overlays did to reflective cracking and better maintenance of the original thickness of the pavement.