This paper considers the influence of thickness of multilayered nano-structured coatings Ti-TiN-(TiCrAl)N and Zr-ZrN-(ZrCrNbAl)N on tool life of metal cutting tools at various cutting speeds (vc = 250, 300, 350 and 400 m·min−1). The paper investigates the basic mechanical parameters of coatings and the mechanism of coating failure in scratch testing depending on thickness of coating. Cutting tests were conducted in longitudinal turning of steel C45 with tools with the coatings under study of various thicknesses (3, 5, and 7 µm), with an uncoated tool and with a tool with a “reference” coating of TiAlN. The relationship of “cutting speed vc—tool life T” was built and investigated; and the mechanisms were found to determine the selection of the optimum coating thickness at various cutting speeds. Advantages of cutting tools with these coatings are especially obvious at high cutting speeds (in particular, vc = 400 m·min−1). If at lower cutting speeds, the longest tool life is shown by tools with thicker coatings (of about 7 μm), then with an increase in cutting speed (especially at vc = 400 m·min−1) the longest tool life is shown by tools with thinner coating (of about 3 μm).
This article discusses the influence of the thickness of a nano-structured wear-resistant layer of the Ti–TiN–(Ti,Al,Si)N multilayer composite coating on its mechanical and performance properties. The study was focused on the coatings with the following thicknesses of its wear-resistant layers: 2, 3.5, 5, 7, 11, and 15 μm. The relation between the thickness of a wear-resistant layer and the time of its deposition was investigated, and the effect of the above thickness on hardness and wear resistance in scratch testing was considered. Cutting tests were conducted in turning steel C45 with carbide inserts with the coatings under study at various cutting speeds (vc = 250, 300 and 350 m/min). The study found the value of thickness of wear-resistant layer providing the longest tool life at various cutting speeds. The differences in the nature of wear for the coatings with various thicknesses of wear-resistant layers were considered.