The article discusses the influence of the thickness of the wear-resistant layer of the Zr-ZrN-(Zr,Al,Si)N nanolayer composite coating on the values of residual stress and the nature of coating wear. The study focused on coatings with wear-resistant layer thicknesses of 2.0, 4.3, 5.9, and 8.5 µm, deposited using filtered cathodic vacuum arc deposition (FCVAD) technology. The X-ray diffraction (XRD) method based on the anisotropy of the elasticity modulus was used to find the values of the residual stress. The nature of the formation of interlayer delamination under the influence of residual compressive stress was studied using a scanning electron microscope (SEM). When the wear-resistant layers had a thickness of 2.0–5.9 μm, tensile stress formed, which decreased with an increase in the thickness of the coating. When the thickness of a wear-resistant layer was 8.5 μm, compressive stress formed. Under the action of compressive stress, periodic interlayer delamination formed, with a pitch of about 10 binary nanolayers. A mathematical model is proposed to describe the nature of the formation of interlayer delamination under the influence of compressive residual stress, including in the presence of a microdroplet embedded in the coating structure.
This article discusses the influence of the thickness of a nano-structured wear-resistant layer of the Ti–TiN–(Ti,Al,Si)N multilayer composite coating on its mechanical and performance properties. The study was focused on the coatings with the following thicknesses of its wear-resistant layers: 2, 3.5, 5, 7, 11, and 15 μm. The relation between the thickness of a wear-resistant layer and the time of its deposition was investigated, and the effect of the above thickness on hardness and wear resistance in scratch testing was considered. Cutting tests were conducted in turning steel C45 with carbide inserts with the coatings under study at various cutting speeds (vc = 250, 300 and 350 m/min). The study found the value of thickness of wear-resistant layer providing the longest tool life at various cutting speeds. The differences in the nature of wear for the coatings with various thicknesses of wear-resistant layers were considered.
The article deals with the problems of cracking in the structure of multilayered coatings under the conditions of stochastic loading process. A mathematical model has been proposed in order to predict the crack propagation velocity in the coating while taking the influence of interlayer interfaces into account. A technique for calculating the probability density distribution of the coating fracture (failure rate) has been developed. The probability of a change in the crack growth direction is compared with the experimental data that were obtained as a result of the studies focused on the pattern of cracking in the Zr,Nb-(Zr,Nb)N-(Zr,Nb,Al)N and Ti-TiN-(Ti,Cr,Al)N coatings under the conditions of the real stochastic loading of cutting tools during the turning. The influence of the crystalline structure of the coating on the cracking pattern has been studied. The investigation has found the significant effect of the crystalline structure of the coating layers on the cracking pattern.
The paper presents the results of studies focused on the specific features typical for the formation of the shape and structure of microdroplets embedded into the structure of the Ti–TiN–(Ti,Cr,Mo,Al)N and Ti–TiN–(Ti,Al,Nb,Zr)N coatings during their deposition. Three main microdroplet shapes—a sphere, a tear, and a lens—have been considered. The specific features typical for the formation of secondary layered structures on the surface of some microdroplets have also been examined. As a result of the conducted investigations, with the use of scanning and transmission electron microscopy, the influence of microdroplets on the distortion of the nanolayer structure of the coatings was studied. A hypothesis has been proposed concerning a relationship between the microdroplet shape and the presence or absence of secondary structures and the microdroplet sizes and weight, as well as the conditions in the unit chamber during the movement of a microdroplet from a cathode to the deposition surface. Based on the study focused on the shape of the microdroplet core and the specific features typical for the formation of the secondary structure around it, a hypothesis has been proposed, according to which, for some microdroplets, it takes much more time than previously assumed for the movement from a cathode to the deposition surface.
The study deals with an increase in the tool life parameter for metal-cutting tools and efficiency of end milling for titanium alloys, due to the use of tools with multilayered composite nano-structured Zr–ZrN–(Zr,Al)N and Zr–ZrN–(Zr,Cr,Al)N coatings, deposited through the technology of the filtered cathodic vacuum arc deposition (FCVAD). The studies included the microstructured investigations using SEM, the analysis of chemical composition (Energy-dispersive X-ray spectroscopy, EDXS), the determination of the value of critical failure force (with the use of scratch testing), and the measurement of the microhardness of the coatings under study. The cutting tests were conducted in end milling of titanium alloys at various cutting speeds. The mechanisms of wear and failure for end milling cutters with the coatings under study were studied in milling. The studies determined the advantages of using a tool with the coatings under study compared to an uncoated tool, as well as to tools with the commercial Ti–TiN coating and the nano-structured Ti–TiN–(Ti,Al)N coating. Adding Cr to the composition of the coating can significantly increase the hardness, while the coating retains sufficient ductility and brittle fracture resistance, which allows for a best result when milling titanium alloys.
This article compares the properties of the diamond-like carbon (DLC) coating with those of ZrN and (Zr,Hf)N coatings deposited on the Ti-6Al-4V titanium alloy substrate. To improve substrate adhesion during the deposition of the DLC coating, preliminary etching with chromium ions was conducted, ensuring the formation of a chromium-saturated diffusion surface layer in the substrate. A Si-DLC layer followed by a pure DLC layer was then deposited. The hardness of the coatings, their surface morphology, fracture strength in the scratch test, and tribological properties and wear resistance in the pin-on-disk test in contact with Al2O3 and steel indenters were investigated. The structure of the DLC coating was studied using transmission electron microscopy, and its corrosion resistance in an environment simulating blood plasma was also investigated. In the pin-on-disk test in contact with Al2O3 and AISI 52100 indenters, the DLC-coated sample demonstrates a much lower friction coefficient and significantly better wear resistance compared to the nitride-coated and uncoated samples. Both nitride coatings—(Zr,Hf)N and ZrN—and the DLC coating slow down the corrosive dissolution of the base compared to the uncoated sample. The corrosion currents of the (Zr,Hf)N-coated samples are 37.01 nA/cm2, 20% higher than those of the ZrN-coated samples. The application of (Zr,Hf)N, ZrN, and DLC coatings on the Ti-6Al-4V alloy significantly inhibits dissolution currents (by 30–40%) and increases polarization resistance 1.5–2.0-fold compared to the uncoated alloy in 0.9% NaCl at 40 °C. Thus, the DLC coating of the described structure simultaneously provides effective wear and corrosion resistance in an environment simulating blood plasma. This coating can be considered in the manufacture of medical products (in particular, implants) from titanium alloys, including those functioning in the human body and subject to mechanical wear (e.g., knee joint endoprostheses).