1 March 2019 in Journal of Power Sources
29 August 2019 in ACS Sustainable Chemistry & Engineering
This research presents a sustainable approach for the simultaneous recycling of spent lithium-ion batteries (LIBs) and nickel-metal hydride batteries (NiMHs). Firstly, dissolution of LIBs and NiMHs were found to be mutually co-promoted, resulting in above 98% extraction of Li, Co, Ni and rare earth elements (REEs) without the need for any oxidant or reductant additions. After leaching, > 97% of REEs were recovered as a REEs-alkali double sulfate precipitate with the addition of NaOH and Na2SO4 precipitants. This REEs-free solution was then further processed in order to separate and recover the battery metals present: Mn, Co, Ni and Li. The resultant residual solution (rich in NaOH and Na2SO4) was redirected to the REEs precipitation step, decreasing both the need of precipitants (e.g. Na2SO4) as well as the costs related to the treatment of the high-Na waste solution. Moreover, the Li remaining in the waste solution can be circulated back into the main process, resulting in an exceptionally high Li recovery of > 93% in the form of high-purity Li3PO4 (99.95%). This is a marked improvement over the previously reported Li recovery levels of 60% - 80%. Overall, this newly developed process has considerable environmental and economic advantages for the recovery of valuable metals from mixed LIBs and NiMHs wastes
1 February 2020 in Journal of Power Sources
1 May 2019 in Hydrometallurgy
19 September 2019 in ACS Sustainable Chemistry & Engineering
In order to achieve the global goals related to renewable energy and responsible production, technologies that ensure the circular economy of metals and chemicals in recycling processes are a necessity. The recycling of spent Nd-Fe-B magnets typically results in rare earth elements (REEs) free wastewaters that have a high ferric ion concentration as well as oxalate groups and for which, there are only a few economically viable methods for disposal or reuse. The current research provides a new approach for the effective recovery of oxalic acid and the results suggest that during the initial oxalate groups separation stage, > 99% of oxalate ions can be precipitated as ferrous oxalate (FeC2O4·2H2O) by an ultrasound-assisted iron powder replacement method (Fe/Fe(III) = 2, tu/s = 5 min, T = 50 °C). Subsequently, almost all of the FeC2O4·2H2O was dissolved using 6 mol/L HCl (T = 65 °C, t = 5 min) and the dissolved oxalates were found to mainly exist in form of H2C2O4. Furthermore, over 80% of the oxalic acid was recovered via crystallization by cooling the oxalate containing HCl solution to 5 °C. After oxalic acid crystallization, the residual raffinate acid solution can then be recirculated back to the ferrous oxalate leaching stage, in order to decrease any oxalic acid losses. This treatment protocol for high iron REEs-free solution not only avoids the potential harm to the environment due to the wastewater but also significantly improves the circular economy of chemicals in the typical utilized in permanent magnet recycling processes.