Based on the advantage of rapid net-shape fabrication, laser powder bed fusion (LPBF) is utilized to process B4C-reinforced Ti composites. The effect of volumetric energy density (VED) on the relative density, microstructural evolution, tensile properties and wear behaviors of B4C-reinforced Ti composites were systematically investigated. The LPBF-ed samples with high relative density (>99%) can be achieved, while the pores and un-melted powders can be observed in the sample owing to the low energy input (33 J/mm3). The additive particulates B4C were transformed into needle-like TiB whiskers with nano-scale while C dissolved in the Ti matrix. Fine-scale grains (<10 μm) with random crystallographic orientation can be achieved and the residual stress shows a downtrend as the VED increases. Through the analysis of the tensile and wear tests, the sample at 61 J/mm3 VED showed a good combination of strength and wear performance, with an ultimate tensile strength of 951 MPa and a wear rate of 3.91 × 10−4 mm3·N−1m−1. The microstructural evolution in VED changes and the corresponding underlying strengthening mechanisms of LPBF-ed Ti + B4C composites are conducted in detail.
Cracking represents a critical issue in γ’-strengthened Ni-based superalloys processed via laser powder bed fusion. This study systematically investigated the influence of scan speed (800–1200 mm/s) on the crack elimination mechanism, microstructural evolution, and mechanical properties of LPBF-processed IN738LC alloy. Near-defect-free IN738LC parts were successfully produced with a relative density of 99.6% and a crack density of only 0.025%. The results indicate that as the scan speed increased from 800 mm/s to 1100 mm/s, a flatter melt pool (S4) was obtained, which reduced the proportion of high-angle grain boundaries. The cooling rate also increased from 13.68 K/μs to 15.96 K/μs, promoting grain refinement and the dispersion precipitation of MC carbides. The refined grains effectively suppressed stress concentration and inhibited crack propagation along grain boundaries. The optimized process (1100 mm/s) achieved optimal comprehensive mechanical properties. Compared to a scan speed of 800 mm/s, the ultimate tensile strength, yield strength, and elongation at room-temperature increased from 1075 MPa, 820 MPa, and 13.2% to 1179 MPa, 871 MPa, and 21.1%, respectively, while hardness increased from 365 HV1.0 to 387 HV1.0. This study demonstrated that the microstructure and mechanical properties of LPBF-processed IN738LC alloy can be tailored via controlling the thermal history of the melt pool, providing a foundation for processing high-crack-sensitivity alloys utilizing laser powder bed fusion.