High quality Ru, Ir, Pd, Pt, Ag, and Au Schottky contacts (SCs) were fabricated on β-Ga2O3 single crystal substrates via rf sputtering under inert and oxidizing plasma conditions. The oxidized SCs exhibited significantly higher rectifying barriers and, with the exception of gold oxide, significantly improved high temperature performance, with more than 12 orders of magnitude of stable rectification at 180 °C. With the exception of Ag, the image-force-corrected laterally homogeneous barrier heights of the plain metal SCs were pinned close to 1.3 eV, irrespective of the metal work function, with the Fermi level at the SC interface close to the predicted VO (2+/0) transition level of fourfold coordinated oxygen vacancies. The equivalent barrier heights of the oxidized SCs were consistently 0.5–0.8 eV higher than their plain metal counterparts, lying in the range of 1.8–2.5 eV, with the increase attributed to the passivation of interfacial oxygen vacancies and a significant increase in the work function of the oxidized metals. The highest Schottky barriers for both the plain and oxidized metal SCs involved Ag, which may be linked to the relative ease of its unintentional and intentional oxidation, respectively. The very high rectifying barriers and the thermal stability of oxidized Schottky contacts to β-Ga2O3 indicate their potential for high temperature device applications.
Oxidized Ir, Pd, Pt, Ag, and Au Schottky contacts (SCs) were fabricated on (010) β-Ga2O3 single crystal substrates via reactive rf sputtering using an O2:Ar plasma. The use of in-situ oxidizing conditions resulted in SCs with very high rectifying barriers in excess of 2.0 eV for all the metals investigated, representing an increase of 0.4 to 0.9 eV compared to the corresponding plain metal versions. Both the plain and oxidized metal SCs showed evidence of Fermi Level pinning with their laterally homogeneous barrier heights lying in narrow ranges of ~1.3 to 1.5 eV and ~2.2 to 2.4 eV, respectively, with little correlation with metal work function. This was attributed to the influence of metal-induced oxygen vacancies and gap states at the SC interface, respectively. The very high barriers of the oxidized SCs resulted in excellent high temperature performance with ~10 orders of magnitude of rectification at 180°C, indicating the potential of this technique for the fabrication of high temperature unipolar devices.
Very high temperature operation β-Ga2O3 Schottky contacts were fabricated on moderately doped β-Ga2O3 single crystal substrates using four different types of intentionally oxidized platinum group metal (PGM) Schottky contacts (SCs), i.e., PtOx, IrOx, PdOx, and RuOx (x ∼ 2.0, 2.2, 1.1, and 2.4, respectively) formed by reactive rf sputtering of plain-metal targets in an oxidizing plasma. All four types of oxidized PGM SCs showed rectification ratios (at ± 3 V) of more than 10 orders of magnitude up to 300 °C, with almost no measurable increase in reverse leakage current density (Jrev) from that at room temperature. From 350 to 500 °C, a measurable increase in Jrev was observed, which was consistent with the thermionic emission of charge carriers over the respective image force (IF) lowered Schottky barriers. Despite this increase, PtOx(IrOx)[PdOx]{RuOx} SCs showed large rectification ratios (at ± 3 V) of 6 × 106(8 × 106)[5 × 105]{2 × 104} and IF-corrected barrier heights of 2.10(2.10)[1.90]{1.60} ± 0.05 eV, respectively, while operating at 500 °C. The significantly lower 500 °C barrier height of the RuOx SCs was due to the thermal reduction of RuOx to Ru that occurred above 400 °C. In contrast, the Schottky barriers of IrOx, PtOx, and PdOx SCs were thermally stable while operating at 500 °C, indicating significant potential for their use in very high temperature rectifying devices.
High-temperature β-Ga2O3 Schottky diodes with very low leakage currents, capable of sensitive UVC detection at 350 °C, were fabricated on (201) β-Ga2O3 single crystal substrates using intentionally-oxidized ruthenium (RuOx) Schottky contacts (SCs), with x = ∼2.1. These RuOx:β-Ga2O3 SCs were characterized by rectification ratios of more than 1010 at ± 3 V and very low reverse leakage current densities of less than 1 nAcm-2 (∼1 pA) at.3.0 V, that were unchanged from 24 to 350 °C. These very low high-temperature leakage currents were due to their extremely high Schottky barriers of 2.2 eV at 350 °C, that were stable against repeated operation at this temperature. Although not optimized for photodetection, these SCs could detect UVC (λ = 248 nm) radiation at a temperature of 350 °C with a UVC/dark current ratio of ∼103. The very high and thermally stable rectifying barriers of these RuOx:β-Ga2O3 SCs makes them strong candidates for use in high temperature β-Ga2O3 rectifying diodes and UVC photodetectors.
Oxidized iridium (IrOx) Schottky contacts (SCs) with excellent high temperature stability were fabricated on β-Ga2O3 single crystal substrates. These IrOx:β-Ga2O3 SCs were operated at temperatures from 24 to 350 °C with only a very small increase in reverse leakage current, while maintaining extremely high rectification ratios (at ±3 V) of more than 10 orders of magnitude at all temperatures, including 350 °C. This remarkable high temperature performance was due to their very high and thermally stable rectifying barriers that, after an initial heat-related improvement, were characterized by zero-bias effective barrier heights of 2.05 ± 0.02 eV and ideality factors of 1.05–1.10, which were almost unchanged by further repeated operation at 350 °C. The reverse leakage current density at 350 °C was only ∼2.3 × 10−9 A cm−2 (∼3.0 pA) at −3 V and ∼7.5 × 10−8 A cm−2 (∼100 pA) at −100 V. These IrOx:β-Ga2O3 SCs represent a significant improvement in high-temperature β-Ga2O3 SC performance, with considerable potential for the fabrication of high temperature β-Ga2O3 rectifying diodes, deep UV photodetectors, and metal-semiconductor field effect transistors.
8 March 2021 in IEEE Transactions on Electron Devices
β-Ga 2 O 3 is a candidate for high-efficiency power electronics and ultraviolet C (UVC) detectors capable of operating in harsh environments. However, electrical contacts that maintain their performance at high temperatures are likely to be important due to the material's low thermal conductivity. In this study, we report on a dramatic improvement in the rectifying performance of Pd Schottky contacts (SCs) on ( -201) and (010) β-Ga 2 O 3 at high temperatures in air. This effect involves a large thermally activated increase in the image-force-corrected barrier height ( Φ B,IF ) from 1.40 eV at room temperature (RT) to 1.75-2.20 eV, with most of the transition occurring between 250 °C and 450 °C. This improvement is due to the oxidation of the Pd SC layer that creates higher barrier height PdO regions that dominate the high-temperature current transport. In the most oxidized Pd SCs, Φ B,IF increased to 2.20 eV at 500 °C with leakage currents of ~ 1×10 -6 Acm -2 (-3 V) and rectification ratios (±3 V) of ~ 10 7 , at 500 °C, similar to the best results for diamond and SiC SCs. Interestingly, very good agreement between the temperature dependence of the built-in voltage of the thermally oxidized Pd SCs and the optical bandgap of β-Ga 2 O 3 (approximately -1.3 meV/°C in both cases) was observed between RT and 500 °C.