Tina Maleki

Tina Maleki

Auto-generated profile, based on publicly available information

Tina Maleki

Department of Prosthetic Dentistry, University Hospital, LMU Munich, Munich, Germany

Research Focus & Metrics

Academic Career Length

3Years (2024-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
12 June 2024 in Dental Materials
Verified
Journal Article
Open access
TMTina Maleki
Tina Maleki
JMJohn Meinen
John Meinen
ACAndrea Coldea
Andrea Coldea
MRMarcel Reymus
Marcel Reymus
DEDaniel Edelhoff
Daniel Edelhoff
BSBogna Stawarczyk
Bogna Stawarczyk
To investigate the flexural strength (FS), elastic modulus (E), Martens hardness (HM), water sorption (wsp), water solubility (wsl) and degree of conversion (DC) of 3D-printed, milled and injection molded splint materials. Specimens (N = 1140) were fabricated from five 3D-printed (GR-22 flex, GR-10 guide, ProArt Print Splint clear, V-Print Splint, V-Print Splint comfort), five milled (BioniCut, EldyPlus, ProArt CAD Splint clear, Temp Premium Flexible, Thermeo) and two injection molded (PalaXPress clear, Pro Base Cold) materials. FS, E, HM, wsp, wsl and DC were tested initially (24 h, 37 °C, H2O), after water storage (90 d, 37 °C, H2O) as well as after thermal cycling (5000 thermal cycles, 5/55 °C). Data were analyzed with Kolmogorov-Smirnov, Kruskal- Wallis, Mann-Whitney U test and Spearman's correlation (p < 0.05). Initially, the mean flexural strength values ranged from 1.9 to 90.7 MPa for printed, 3.8 to 107 MPa for milled and 99.7 to 102 MPa for injection molded materials. The initial mean elastic modulus values were 0.0 to 2.4 GPa for printed, 0.1 to 2.7 GPa for milled and 2.8 GPa for injection molded materials. The initial mean Martens hardness values were 14.5 to 126 N/mm2 for printed, 50.2 to 171 N/mm2 for milled and 143 to 151 N/mm2 for injection molded materials. Initially, the mean water sorption values ranged from 23.1 to 41.2 μg/mm3 for printed, 4.5 to 23.5 μg/mm3 for milled and from 22.5 to 23.3 μg/ mm3 for injection molded materials. The initial mean water solubility values ranged from 2.2 to 7.1 μg/mm3 for printed, 0.0 to 0.5 μg/mm3 for milled and 0.1 to 0.3 μg/mm3 for injection molded materials. After water storage and thermal cycling most of the values decreased and some increased. The mean DC values ranged initially from 72.3 to 94.5 %, after water storage from 74.2 to 96.8 % and after thermal cycling from 75.6 to 95.4 % for the printed materials. The mechanical and physical properties of printed, milled and injection molded materials for occlusal devices vary and are influenced by aging processes. For clinical applications, materials need to be chosen according to the specific indications.

6 May 2025 in Clinical Oral Investigations
Verified
Journal Article
Open access
PDF file
TMTina Maleki
Tina Maleki
ACAndrea Coldea
Andrea Coldea
JMJohn Meinen
John Meinen
MRMarcel Reymus
Marcel Reymus
DEDaniel Edelhoff
Daniel Edelhoff
BSBogna Stawarczyk
Bogna Stawarczyk
Objectives: To investigate the torque load (TL) and angular rotation (AR) of additively, subtractively and conventionally manufactured occlusal devices. Materials and methods: Specimens (N = 120) were fabricated from four additive manufacturing resins (GR-10 guide, ProArt Print Splint clear, V-Print Splint, V-Print Splint comfort), five subtractively (BioniCut, EldyPlus, ProArt CAD Splint clear, Temp Premium Flexible, Thermeo) and one conventionally manufactured (Pro Base Cold) materials. The TL and AR were tested initially (24 h, 37 °C, H2O) as well as after thermal cycling (5,000 thermal cycles, 5/55°C). Data were analyzed using Kolmogorov–Smirnov, one-way ANOVA, Scheffé post-hoc, t-test, chi-square and Ciba-Geigy table (p < 0.05). Results: Initially, the mean TL values ranged from 63.7 to 104 Ncm for additively, 39.2 to 265 Ncm for subtractively, and 204 Ncm for conventionally manufactured materials. The initial mean AR values were 41.7 to 143 deg for additively, 38.4 to 138 deg for subtractively, and 29.3 deg for conventionally manufactured materials. After thermal cycling, the mean TL values ranged from 45.7 to 88.1 Ncm for additively, 31.2 to 246 Ncm for subtractively, and 138 Ncm for conventionally manufactured materials. The mean AR values after aging ranged from 19.9 to 124 deg for additively, 48.1 to 131 deg for subtractively, and 19.5 deg for conventionally manufactured materials. Conclusions: The torsional resistance of additively, subtractively, and conventionally manufactured materials for occlusal devices varies and is affected by aging processes. Clinical Relevance: Material selection for occlusal devices should be guided by the clinical needs of the patients.