Bamboo is a naturally occurring composite material, which exhibits a decomposable structure with varying composition. The distinct structural features of bamboo contribute to its exceptional strength and flexibility, making it an excellent choice for construction purposes. However, only a limited portion of bamboo species has been studied for its mechanical properties, and research on Bambusa arundinaceae has primarily focused on its pharmaceutical values. Therefore, we investigated the relationship between the structural characteristics of B. arundinaceae and its mechanical properties using axial compression experiments and tangential bending experiments. The results showed that the distribution density of vascular bundles (VBs) of B. arundinaceae ranged from 1.98 to 4.34 pcs/mm2,while the volume fraction of fiber sheaths (FSs) ranged from 35.82 to 42.58%. The average compressive strength, flexural strength, and flexural elasticity modulus were 113.99 MPa, 239.07 MPa, and 17.39 GPa, which were 97.56%, 64.07%, and 66.09% higher than those of moso bamboo (Phyllostachys edulis), respectively. The compressive strength, flexural strengths, and elasticity modulus of B. arundinaceae were positively correlated with both the distribution density of VBs and the volume fraction of FSs. These insights are crucial for the advancement of durable and efficient materials in diverse sectors including construction and manufacturing.
Calamus caesius is one of the most well-known commercial climbing palm species across the world. A comprehensive understanding of the growth-dependent variation in microstructure and polymer distribution can provide fundamental information to guide its end-use applications. In this study, we investigated the age-wise characteristics of rattan stems and the ultrastructure of fibers using electron microscopy, light microscopy, and FTIR. The results showed that the frequency of vascular bundles with a diameter of 0.55∼0.62 mm in C. caesius was 3.49∼3.97 pieces/mm. The diameter and length of the metaxylem vessel were 0.32∼0.34 mm and 2.86∼3.00 mm, respectively. Cellulose, lignin, xylan, and HCA are mainly concentrated in the fiber sheath of vascular bundles. The distribution of major polymers in positions other than the top was relatively stable. The tissue proportion of parenchyma, xylem, and phloem did not differ significantly at different positions. The proportion of fibers from 22.27%∼25.33% showed significant differences. The fiber length was 1.43∼1.76 mm, and the diameter was 10.78∼12.63 m. During the growth process of the rattan stem, the secondary wall of fiber cells continued to accumulate inward towards the cell cavity from 2 to 6 layers. The unique fiber properties and stable vascular bundle composition of C. caesius may have potential in fields such as composite materials or renewable energy.
Unlike the culm hollow structure of most bamboo species, Oxytenanthera abyssinica has a unique solid or semi-solid culm, which may endow it with superior mechanical performance. In this study, the variation in fiber morphology and micro-mechanical properties across the radial regions of bamboo culm was examined by optical microscopy, scanning electron microscopy, X-ray diffraction, and nanoindentation. Results showed that the mean values of vascular bundle frequency and fiber tissue proportion were 1.76 pcs/mm and 21.04%, respectively, both of which increased gradually from inner to outer. The mean length, diameter, and length-diameter ratio of the fiber were 2.10 mm, 21.54 m, and 101.41 respectively. The mean indentation modulus of elasticity (IMOE) and hardness were 21.34 GPa and 545.88 MPa. The IMOE exhibited a significant increase from the inner to the middle region, and little change was observed from the middle to the outer region. There were slight fluctuations in hardness along the radial direction. The mean crystallinity and microfibril angle(MFA) of the fibers was 68.12% and 11.26 degrees, respectively. There is a positive correlation between cellulose crystallinity and the IMOE and hardness, while there is a negative correlation between the MFA and the IMOE and the hardness.