1 January 2006 in Superlattices and Microstructures
8 July 2004 in Physica Status Solidi (a)
1 December 2003 in Physica B: Condensed Matter
27 October 2015 in Journal of Applied Physics
Thin films of monoclinic nanostructured vanadium dioxide are notoriously difficult to produce in a selective manner. To date, post-annealing, after pulsed laser deposition (PLD), has been used to revert the crystal phase or to remove impurities, and non-glass substrates have been employed, thus reducing the efficacy of the transparency switching. Here, we overcome these limitations in PLD by optimizing a laser-ablation and deposition process through optical imaging of the laser-induced plasma. We report high quality monoclinic rutile-type vanadium dioxide (VO2) (M1) nanoparticles without post-annealing, and on a glass substrate. Our samples demonstrate a reversible metal-to-insulator transition at ∼43 °C, without any doping, paving the way to switchable transparency in optical materials at room temperature.
7 January 2002 in Applied Physics Letters
1 March 2015 in Optical Engineering
The effect of an oxygen atmosphere on the expansion dynamics of a laser-produced vanadium-oxygen plasma has been investigated using a fast intensified charged-coupled device camera. We find regimes of the plasma plume expansion ranging from a free plume at vacuum and low oxygen pressures, through collisional and shock-wave-like hydrodynamic regimes at intermediate oxygen pressure, finally reaching a confined plume with subsequent thermalization of the plume particles at the highest pressure of the oxygen gas. Vanadium oxide nanostructures thin films were synthesized from this plasma and the resulting vanadium oxide phases studied as a function of the plume dynamics. We found monoclinic vanadium dioxide (VO2) (M1) and VO2 (B) nanoparticles in thin films deposited at 0.05 mbar. Pure phases of vanadium trioxide (V2O3) smooth and pentoxide (V2O5) nanorods thin films were detected at 0.01 and 0.1 to 0.2 mbar, respectively. Thin films containing VO2 (M1) were found to have a reversible metal-to-insulator transition at 61°C. This work paves the way to VO phase control by judicious choice of laser and plasma conditions.