The object of this research is the pack carburizing of ST 37 low-carbon steel using activated carbon derived from catfish bone waste as a sustainable carburizing medium. ST 37 has low surface hardness, and it is not established how carburizing temperature and holding time govern the resulting hardness and microstructure when a fish-bone-derived carbon is used. Specimens were carburized at 800°C and 875°C for 45, 90, and 115 minutes, followed by water quenching; surface hardness was measured on the Rockwell B scale and the case region was examined by optical microscopy. At 800°C the surface hardness increased from 53.33 to 87.00 HRB as the holding time rose from 45 to 115 minutes, with the case microstructure progressing from ferrite with coarse pearlite to fine pearlite and then to a finer ferrite-carbide constituent. At 875°C the hardness reached 98.33 HRB at every holding time, with the case transforming to a fine, dark-etching ferrite-carbide constituent; this value lies at the upper limit of the Rockwell B scale, so it represents the maximum measurable, not the true, case hardness, and temperature exerted a stronger influence than time. No fully martensitic case formed, which is consistent with the low hardenability of ST 37 and is favorable because hardness is raised without a brittle case. Unlike conventional carburizing that relies on commercial charcoal, the present medium uses fish-bone waste and reaches maximum hardness at 875°C in 45 minutes. These findings apply to small-scale surface hardening of low-carbon steel where fish-bone waste is locally available and a tough, wear-resistant surface is required. The results confirm that catfish bone waste can serve as a low-cost, sustainable carburizing medium for low-carbon steel