A novel hybrid surface-enhanced Raman scattering (SERS) substrate based on Au nanoparticles decorated inverse opal (IO) photonic crystal (PhC) is presented. In addition to the enhancement contributed from Au nanoparticles, a desired Raman signal can be selectively further enhanced by appropriately overlapping the center of photonic bandgap of the IO PhC with the wavelength of the Raman signal. Furthermore, the lattice structure of the IO PhC provides excellent control of the distribution of Au nanoparticles to produce SERS spectra with high uniformity. The new design of SERS substrate provides extra maneuverability for ultra-high sensitivity sensor applications.
1 September 2009 in Journal of Physics: Conference Series
High-quality photonic crystals of SiO2 spheres and air spheres are fabricated using self-assembling processes and infiltration method with thermal-assistant cell method. Their photonic band structures are characterised by reflectivity spectra measurements. It shows that the tunable optical stop bands are determined by refractive index contrast, diameter of spheres and angle of light illumination. The experimental results of reflectivity spectra agree very well with the results obtained by theoretical Bragg diffraction and photonic band calculations.
We present the synthesis of Er3+/ Yb3+ co-doped Gd2O3 nanospheres using the wet-chemical method followed by a synergistic step-by-step calcination process, a novel approach in the field. The nanospheres exhibited red color upconversion luminescence (UCL) after multi-step annealing at temperatures ranging from 650 °C to 1150 °C, achieving a fully spherical morphology. The diameter and surface morphology of the nanospheres were significantly altered by the annealing process, decreasing from 382.77 ± 1.72 nm with a smooth surface to 245.7 ± 1.31 nm with a rougher surface. The UCL intensity increased with the annealing temperature. The influence of Er3+/ Yb3+ co-doped Gd2O3 nanospheres, excited by a 975 nm laser, was investigated, and the decay time for UCL samples was analyzed. The luminescence peak at 1026 nm was attributed to the 4I11/2 (Er3+) + 2F7/2 (Yb3+) → 4I15/2 (Er3+) + 2F5/2 (Yb3+) transition/ or 2F5/2 → 2F7/2 of the Yb3+ ions within the Gd2O3 matrix. Furthermore, the UCL properties of Er3+/ Yb3+ co-doped Gd2O3 nanophosphors were explored to detect the NTERA-2 cancer cells. These findings suggest that the rare earth co-doped Gd2O3 nanospheres might hold significant potential for biomedicine and imaging diagnostics applications, sparking new interest and possibilities in these fields.