The influence of continuous casting and hot rolling (on a broad-strip 2000 mill) on the hot plasticity of microalloyed pipe steel (strength category X42) is investigated. A Gleeble 3800 system is...
31 January 2017 in Transactions of the Indian Institute of Metals
Deform-3D software is used to model surface-crack formation in the rolling of thick sheet on a 5000 mill. The calculations show that the temperature field and stress state are relatively uniform over the width of the sheet, except at the edges. The minimum temperature of the surface layers of metal hardly depends on the sheet thickness and the relative reduction per pass. The Cockroft–Latham criterion is used to analyze the probability of steel failure in rolling. Analysis shows that metal failure may occur at points where ferrite appears, especially at the instant that the metal leaves the deformation region. Considerable tensile stress acts at those points.
The formation of a surface defect (a lobed scab) in the final stage of large-diameter pipe production is analyzed. Surface microcracks are assumed to form in the rolling of thick sheet on account of problems in the two-phase region on rolling, with localization of the plastic strain, as well as the action of tensile stress in the surface layer and the attainment of limiting stress values. Physical modeling in the Gleeble system permits determination of the limiting stress (rupture strength) in rolling in the two-phase region, which depends on the temperature and is structure-sensitive. The limiting stress is determined by ferritic and bainitic transformation in the steel.