We aimed to evaluate the color stability of bulk-fill and conventional composite resin with respect to thickness and storage media. Twenty specimens of a conventional composite resin (6 mm diameter and 2 mm thick) and 40 specimens of the bulk-fill Tetric EvoCeram composite resin at two different thicknesses (6 mm diameter and 2 mm thick or 4 mm thick,) were prepared. The specimens were stored in distilled water during the study period (28 d). Half of the specimens were remained in distilled water and the other half were immersed in coffee solution 20 min/d and kept in distilled water between the cycles. Color changes () were measured using the CIEcolor space and a digital imaging system at 1, 7, 14, and 28 days of storage. Data were analyzed using Two-way ANOVA and Tukey’s HSD post hoc test (). Composite resins showed significant increase in color changes by time (bulk-fill > conventional;). Coffee exhibited significantly more staining susceptibility than that of distilled water (). There was greater color changes with increasing the increment thickness, which was significant at 14 () and 28 d (). Color change of bulk-fill composite resin was greater than that of the conventional one after coffee staining and is also a function of increment thicknesses.
7 May 2021 in International Journal of Dentistry
Aim. Several new bioactive compounds were recently introduced to the market with favorable ion release, tooth remineralization, and alkalizing potential. This study sought to compare the phosphate ion release and alkalizing potential of three bioactive materials in comparison with composite resin. Methods. Thirty-six discs (2×6mm) were fabricated from Fuji II LC resin modified glass ionomer (RMGI), Activa BioActive, Cention N, and Z250 composite in plastic molds. The specimens were stored in distilled water for 24 and 48h and 6 months. Half of the specimens were used to assess the phosphate ion release while the other half were used to assess the alkalizing potential 1h after pH drop from 6.8 to 4. Phosphate ion release was quantified by a spectrophotometer while the pH value was measured by a pH meter. Data were analyzed using two-way ANOVA, one-way ANOVA, and Tukeys HSD test (for pairwise comparisons) at 0.05 level of significance. Results. At 24h, the maximum phosphate ion release in distilled water occurred in the Fuji II LC group followed by Cention N, Activa BioActive, and Z250. At 6months, Cention N followed by Activa BioActive showed higher phosphate ion release than Fuji II LC and Z250. No significant difference was noted between Activa BioActive and Cention N at any time point. All materials, except for Z250, increased the pH of the environment. Fuji II LC had maximum alkalizing effect at all time points followed by Cention N and Activa BioActive. Conclusion. Use of bioactive compounds is a promising method to ensure phosphate ion release, and can have a positive effect on tooth remineralization over time. Also, bioactive compounds can alkalize an acidic environment.
1 January 2020 in Restorative Dentistry & Endodontics
Iravani M, et al. Restor Dent Endod. 2019 Nov;45:e41. /Synapse/10.5395/rde.2020.45.e41
12 April 2021 in International Journal of Biomaterials
This study assessed the effect of addition of aqueous extract of propolis in different concentrations on the mechanical and antimicrobial properties of resin-modified glass ionomer cement (RMGIC). In this in vitro study, powder of Fuji II LC RMGIC was mixed with 25% and 50% aqueous extracts of propolis. Samples (n = 15 for shear bond strength, n = 5 for flexural strength, and n = 20 for the antibacterial activity test) were fabricated using this mixture. The buccal and lingual surfaces of 23 premolars were ground to expose dentin. Tygon tubes were filled with cement, bonded to dentin, and subjected to bond or the flexural strength test in a universal testing machine. Antibacterial activity was assessed using the disc diffusion and well-plate techniques against S. mutans. Data were analyzed using one-way ANOVA and Tukey’s test. The three groups showed significant differences ( < 0.001). The 50% propolis group had the lowest flexural and shear bond strength. The control group had the highest flexural and shear bond strength. No growth inhibition zone was noted around any of the discs. It can be concluded that addition of propolis to RMGIC did not confer any antibacterial activity against S. mutans and decreased the flexural and shear bond strength of RMGIC.
1 January 2020 in Restorative Dentistry & Endodontics
Javid B, et al. Restor Dent Endod. 2019 Nov;45:e3. https://doi.org/10.5395/rde.2020.45.e3
1 January 2022 in Restorative Dentistry & Endodontics
Farzad A, et al. Restor Dent Endod. 2022 Feb;47:e9. https://doi.org/10.5395/rde.2022.47.e9