Bernhard Ungerer

Bernhard Ungerer

Auto-generated profile, based on publicly available information

Bernhard Ungerer

Department of Material Science and Process Engineering, Institute of Wood Technology and Renewable Materials, University of Natural Resources and Life Sciences Vienna, Tulln an der Donau, Austria

Research Focus & Metrics

Academic Career Length

6Years (2021-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
6 May 2024 in Construction and Building Materials
Verified
Journal Article
Closed access
MHMaryam Haseli
Maryam Haseli
DEDavood Efhamisisi
Davood Efhamisisi
AAAli Abdulkhani
Ali Abdulkhani
ROReza Oladi
Reza Oladi
BUBernhard Ungerer
Bernhard Ungerer
UMUlrich Müller
Ulrich Müller

23 March 2024 in Forests
Verified
Journal Article
Open access
PDF file
HAHajir Al-musawi
Hajir Al-musawi
CHChristian Huber
Christian Huber
BUBernhard Ungerer
Bernhard Ungerer
MJMatthias Jakob
Matthias Jakob
MPMax Pramreiter
Max Pramreiter
Ulrich MüllerUlrich Müller
Ulrich Müller
The plastic deformation of wood perpendicular to the grain is gaining increasing importance due to advancements in forming technologies and the densification of wood. This study investigates how two hardwood species, i.e., beech (Fagus sylvatica) and birch (Betula pendula), respond to compression in the radial direction and examines the structural changes they undergo during both elastic and plastic deformation. Stress–strain curves at different moisture contents (dry to wet) and temperature conditions (20 to 140 °C) were recorded. In-situ observations at high moisture content and temperatures by means of different microscopic techniques are practically unfeasible. Therefore, the specimens were analysed ex-situ microscopically after the test. In addition to the compression of transversely oriented fibres and vessels, special attention was paid to the deformation behaviour of the wood rays. The results suggest that the wood ray cells carry a relatively higher proportion of the load in the radial loading direction than the surrounding vessels and fibres. This observation is supported by the higher percentage of deformed vessels, seen in the microscopy, in areas where the rays developed kinks, usually in the early wood of beech and anywhere in the cross-section of birch. The weaving of rays around big vessels introduced shear strains under compressive stresses at the kinked rays’ area. Thus, shear deformation is more evident in early wood than in late wood regions of wood. However, when the wood was tested at elevated moistures and temperatures, the material demonstrated a ductile response, namely the absence of localised shear deformations. Notably, wet beech and birch specimens heated to 100 °C and above exhibited pronounced thickness recovery and there was slightly irreversible buckling of rays and vessel deformations. Therefore, under such conditions, wood behaves like a “sponge” and is expected to be successfully processed without introducing clear damage to the material. This characteristic holds promise for replication in the development of bio-based energy-absorbing materials.

29 November 2021 in Polymer Composites
Verified
Journal Article
Open access
PDF file
BUBernhard Ungerer
Bernhard Ungerer
UMUlrich Müller
Ulrich Müller
MPMaximilian Pramreiter
Maximilian Pramreiter
EAEnrique Herrero Acero
Enrique Herrero Acero
SVStefan Veigel
Stefan Veigel
The present study investigated the effect of selected structural parameters on the mechanical performance of regenerated cellulose composites. The experimental setup comprised continuous viscose (rayon) yarns embedded in a matrix of epoxy resin. Mechanical and microscopic characterizations involved comparing the following: yarns consisting of untwisted filaments and twisted warp and weft yarns taken from a plain weave fabric, yarns with and without avivage (fiber finish), as well as yarns with and without an acrylic coating. During the epoxy treatment, samples were either prestressed or laid horizontally to preserve the original yarn structure. Tensile tests revealed that yarn crimp had a significant impact on the strength properties of composite specimens, a higher crimp ratio leading to a decrease in performance. Applying prestress to crimped yarns has proven to be an effective way to enable straight alignment in the loading direction, which is essential for the design of stiffness‐ and strength‐optimized yarn composites. Unlike an avivage, which did not markedly affect the mechanical properties of composite yarns, the application of an acrylic coating prior to resin impregnation was found to provide significantly increased extensibility and more ductile fracture behavior.

26 April 2025 in Composites Part B: Engineering
Verified
Journal Article
Open access
BUBernhard Ungerer
Bernhard Ungerer
PMPhilipp Matz
Philipp Matz
FKFlorian Kupelwieser
Florian Kupelwieser
HAHajir Al-musawi
Hajir Al-musawi
GPGabriel Praxmarer
Gabriel Praxmarer
UMUlrich Müller
Ulrich Müller

2 June 2021 in Scientific Reports
Verified
Journal Article
Open access
PDF file
BUBernhard Ungerer
Bernhard Ungerer
UMUlrich Müller
Ulrich Müller
APAntje Potthast
Antje Potthast
EAEnrique Herrero Acero
Enrique Herrero Acero
SVStefan Veigel
Stefan Veigel
In the development of structural composites based on regenerated cellulose filaments, the physical and chemical interactions at the fibre-matrix interphase need to be fully understood. In the present study, continuous yarns and filaments of viscose (rayon) were treated with either polymeric diphenylmethane diisocyanate (pMDI) or a pMDI-based hardener for polyurethane resins. The effect of isocyanate treatment on mechanical yarn properties was evaluated in tensile tests. A significant decrease in tensile modulus, tensile force and elongation at break was found for treated samples. As revealed by size exclusion chromatography, isocyanate treatment resulted in a significantly reduced molecular weight of cellulose, presumably owing to hydrolytic cleavage caused by hydrochloric acid occurring as an impurity in pMDI. Yarn twist, fibre moisture content and, most significantly, the chemical composition of the isocyanate matrix were identified as critical process parameters strongly affecting the extent of reduction in mechanical performance. To cope with the problem of degradative reactions an additional step using calcium carbonate to trap hydrogen ions is proposed.

3 April 2025 in Cellulose
Verified
Journal Article
Open access
PDF file
MAMuhammad Sohaib Anas
Muhammad Sohaib Anas
BUBernhard Ungerer
Bernhard Ungerer
HAHajir Al-Musawi
Hajir Al-Musawi
UMUlrich Müller
Ulrich Müller
Fiber-reinforced composite materials have transformed multiple industries because of their outstanding mechanical properties and lightweight characteristics. Glass fiber composites are commonly used in structural applications due to their high strength-to-weight ratio. Researchers are investigating alternative fibers due to concerns about environmental sustainability and manufacturing costs. This study investigates the mechanical properties of composites reinforced with high-strength regenerated cellulose (viscose) tape fabrics, aiming to assess their suitability as alternatives to traditional materials like glass fabric. Three different weave patterns, plain 1/1, twill 2/2, and satin 5/1 were used as reinforcements along with a glass fabric satin 7/1 for comparison. The composites were fabricated using a hand lay-up technique and cured at different levels of pressure. Mechanical testing was conducted to evaluate tensile strength, modulus of elasticity, and work of fracture. The crimp ratio (%) was calculated for each composite type based on microscopy scans of the specimen’s cross-section. Satin weave viscose composites achieve up to 30–35% of the glass fabric composites in case of Modulus and tensile strength. The highest modulus of elasticity recorded for satin weave viscose composites is 10.8 GPa, compared to 29.8 GPa for glass fabric composites. Tensile strength of satin weave viscose composites reaches up to 180 MPa, while glass fabric composites achieve up to 430 MPa. Microscopic examinations demonstrate that as pressure increases, the crimp ratio decreases, and this change in crimp ratio directly impacts stiffness properties. However, the viscose fiber composites tested were inferior to glass fiber composites in terms of stiffness but surpass 40–60% in terms of work of fracture. The potential for improving the mechanical properties can be found in changing the mechanical properties of the viscose and in adapted weave patterns. Graphical abstract