This study aims to deeply understand the effect of contact stress and slip ratio on wear performances of bainitic rail steels. The results showed that the wear loss increased as the contact stress and slip ratio increased. Based on the surface damage morphology and microstructural analyses, it revealed that the rolling contact fatigue wear mechanism played a significant role under the low slip ratio, but the dominant wear mechanism transferred to the abrasive wear at the high slip ratio. Meanwhile, the bainitic steel specifically presented worse wear resistance under the abrasive wear mode. Compared with the influence of a slip ratio, the increase in contact stress led to severer plastic flows and contributed to the propagation of cracks. In addition, the contact stress and slip ratio had the opposite effect on the friction coefficient, that is, the friction coefficient of bainitic steels behaved the inverse proportion with the contact stress, but positive proportion with the slip ratio. At last, the increase in slip ratio had more significant effect on the reduction of retained austenite (RA) than the enlargement of contact stress due to the fact that the RA would probably be removed before the martensitic transformation occurred under the abrasive wear mechanism.
The effects of cyclic loading on the surface microstructure evolution of different contact locations in a used pearlitic rail were studied. Microstructures were analyzed using Scanning Electron Microscopy (SEM). Meanwhile, grain boundaries and crystallographic orientations were explored via Electron Backscatter Diffraction (EBSD). At last, wheel–rail contact probabilities and forces were calculated using rail profiles. The results indicate that the side wear region located in the gauge face was 71.5% in the high-angle grain boundaries (HAGBs) fraction, 0.88 in the Kernel Average Misorientation (KAM) value, 36% in the recrystallization (REX) fraction, and had a predominant orientation in grains. The rolling contact fatigue (RCF) region situated at the gauge corner was 66.3% in the HAGBs fraction, 0.92 in the KAM value, 33% in the REX fraction, and was mis-orientated in grains. The region located at the edge of the running band was 60.7% in the low-angle grain boundaries (LAGBs) fraction, 0.97 in the KAM value, 12% in the REX fraction, and was mis-orientated in grains. Continuous dynamic recrystallization (cDRX) took place in wear and RCF regions during the cyclic rolling contact loading, creating ultra-fine grains with a transformation from LAGBs to HAGBs, lower KAM values, and more REX. Grains oriented along [111] parallel to the vertical direction in the wear region were influenced by the dominant normal force, while grains in the RCF region were non-oriented, which was attributed to large lateral and vertical forces of similar magnitudes.