In clinical practice, hydroxyapatite (HA) cements for bone defect treatment are frequently prepared by mixing a powder component and a liquid component shortly before implantation in the operation theater, which is time‐consuming and error‐prone. In addition, HA cements are only slightly resorbed, that is, cement residues can still be found in the bone years after implantation. Here, these challenges are addressed by a prefabricated magnesium phosphate cement paste based on glycerol, which is ready‐to‐use and can be directly applied during surgery. By using a trimodal particle size distribution (PSD), the paste is readily injectable and exhibits a compressive strength of 9–14 MPa after setting. Struvite (MgNH 4 PO 4 ·6H 2 O), dittmarite (MgNH 4 PO 4 ·H 2 O), farringtonite (Mg 3 (PO 4 ) 2 ), and newberyite (MgHPO 4 ·3H 2 O) are the mineral phases present in the set cement. The paste developed here features a promising degradation of 37% after four months in an ovine implantation model, with 25% of the implant area being newly formed bone. It is concluded that the novel prefabricated paste improves application during surgery, has a suitable degradation rate, and supports bone regeneration.
Magnesium phosphate-based bone cements, particularly struvite (MgNH4PO4∙6H2O)-forming cements, have attracted increased scientific interest in recent years because they exhibit similar biocompatibility to hydroxyapatite while degrading much more rapidly in vivo. However, other magnesium-based minerals which might be promising are, to date, little studied. Therefore, in this study, we investigated three magnesium-based bone cements: a magnesium oxychloride cement (Mg3(OH)5Cl∙4H2O), an amorphous magnesium phosphate cement based on Mg3(PO4)2, MgO, and NaH2PO4, and a newberyite cement (MgHPO4·3H2O). Because it is not sufficiently clear from the literature to what extent these cements are suitable for clinical use, all of them were characterized and optimized regarding setting time, setting temperature, compressive strength and passive degradation in phosphate-buffered saline. Because the in vitro properties of the newberyite cement were most promising, it was orthotopically implanted into a partially weight-bearing tibial bone defect in sheep. The cement exhibited excellent biocompatibility and degraded more rapidly compared to a hydroxyapatite reference cement; after 4 months, 18% of the cement was degraded. We conclude that the newberyite cement was the most promising candidate of the investigated cements and has clear advantages over calcium phosphate cements, especially in terms of setting time and degradation behavior.
Low back pain is among the main issues in vertebral orthopaedics. Intervertebral disk degeneration can be severe, up to requiring the replacement of the damaged disk by substitutes to achieve spine fusion. Disk removal results in critical size defects, so fusion does not occur naturally, but synthetic bone grafts are needed. Since the surgical procedure is time‐consuming, high infection rates occur. Hence, in spine fusion, bone regeneration enhancement and infection prevention are needed. Here, a new dual‐component system is proposed, to tackle both issues at one time. To enable spine fusion, 3D extrusion‐based printing is employed to develop coherent custom magnesium phosphate (CaMgP)‐based cages. The 3D‐printed scaffolds are hardened, and the structural properties are evaluated to be within the ranges of physiological bone. To prevent infection, an in‐house ice‐templating device is employed in combination with a 3D‐printed ceramic scaffold, to develop tailored porous alginate structures loaded with vancomycin. Results show that CaMgP can be printed into complex geometries and that the geometry influences the pore orientation during ice‐templating. These structures loaded with vancomycin have antibacterial properties against Escherichia coli (E. coli) and Staphylococcus aureus (S. aureus) strains.
Biofilm-driven peri-implant diseases remain a major challenge in implantology. Implant surfaces that promote soft-tissue sealing while limiting bacterial adhesion are essential for establishing a stable biological barrier. In this study, we systematically investigated the effects of topography, surface energy, and surface chemistry on oral cell behavior and biofilm formation using chemically modified and nanodiamond (ND)-functionalized titanium surfaces. Hydroxylated NDs with different aggregate sizes (~50–100 nm) were immobilized on polished commercially pure titanium by electrochemical anodization. Selected surfaces were additionally functionalized with 3‑aminopropyltriethoxysilane (APTES) or 1H,1H,2H,2H-Perfluorooctyltriethoxysilane (PFOS). Cross-sectional analysis confirmed stable partial integration of NDs within the anodic TiO2 layer. Surface characterization revealed three distinct roughness levels and two wettability regimes, with hydroxyl-ND and APTES surfaces remaining hydrophilic and PFOS surfaces becoming hydrophobic.ND-coated surfaces consistently enhanced fibroblast number and spreading independent of surface chemistry, indicating a dominant effect of nanoscale topography. Keratinocytes, however, exhibited greater sensitivity to surface chemistry, preferentially adhering to nano-rough surfaces characterized by hydrophilic and neutrally charged properties. Biofilm formation showed no significant differences between surface variants after saliva conditioning, suggesting masking effects of the salivary pellicle. Overall, ND-modified titanium surfaces show potential for improving soft-tissue integration without increasing biofilm accumulation.