17 July 1995 in Applied Physics Letters
Monocrystalline GaN(0001) thin films, void of oriented domain structures and associated low-angle grain boundaries, have been grown via organometallic vapor phase epitaxy (OMVPE) on high-temperature monocrystalline AlN(0001) buffer layers predeposited on vicinal α(6H)–SiC(0001) wafers using TEG, TEA, and ammonia in a cold wall, vertical, pancake-style reactor. The surface morphology was smooth, and the PL spectrum showed strong near-band-edge emission with a full width at half-maximum (FWHM) value of 4 meV. The dislocation density within the first 0.5 μm was ≊1×109 cm−2; it decreased substantially with increasing film thickness. Controlled n-type Si doping of GaN has been achieved for net carrier concentrations ranging from ∼1×1017 to 1×1020 cm−3. Double-crystal XRC measurements indicated a FWHM value of 66 arcsec for the GaN(0004) reflection.
12 July 1999 in Applied Physics Letters
Pendeoepitaxy, a form of selective lateral growth of GaN thin films has been developed using GaN/AlN/6H–SiC(0001) substrates and produced by organometallic vapor phase epitaxy. Selective lateral growth is forced to initiate from the GaN sidewalls of etched GaN seed forms by incorporating a silicon nitride seed mask and employing the SiC substrate as a pseudomask. Coalescence over and between the seed forms was achieved. Transmission electron microscopy revealed that all vertically threading defects stemming from the GaN/AlN and AlN/SiC interfaces are contained within the seed forms and a substantial reduction in the dislocation density of the laterally grown GaN. Atomic force microscopy analysis of the face of discrete pendeoepitaxial structures revealed a root mean square roughness of 0.98 Å. The pendeoepitaxial layer photoluminescence band edge emission peak was observed to be 3.454 eV and is blueshifted by 12 meV as compared to the GaN seed layer.
16 September 1998 in Applied Physics Letters
Single crystalline (0001) gallium nitride layers were implanted with beryllium. Photoluminescence (PL) measurements were subsequently performed as a function of implantation dose and annealing temperature. One new line in the PL spectra at 3.35 eV provided strong evidence for the presence of optically active Be acceptors and has been assigned to band–acceptor (eA) recombinations. The determined ionization energy of 150±10 meV confirmed that isolated Be has the most shallow acceptor level in GaN. Co-implantation of nitrogen did not enhance the activation of the Be acceptors.
1 April 1996 in Journal of Materials Research
19 May 1997 in Nuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms
27 April 2017 in Physica Status Solidi (b)