1 December 2017 in Journal of Alloys and Compounds
29 July 2019 in Metals and Materials International
1 July 2018 in Key Engineering Materials
ECEduardo Sanchez Caballero
Eduardo Sanchez Caballero
This paper focuses on the microstructural characterization of Al25Ti75, Al37Ti63, Al50Ti50, Al63Ti37and Al75Ti25powders mixtures prepared by mechanical alloying (MA). The high-energy ball-milling, up to 75 h, of aluminium and titanium powders leads to a nanocrystalline or an amorphous structure. It is showed that a stable amorphous Al–Ti phase with uniform elemental distribution forms after 50 h of milling in Al50Ti50alloy. Heat treatment of the different alloys leads to the crystallization of AlTi3, AlTi, Al2Ti and Al3Ti intermetallic compounds. A comprehensive study by laser granulometry, X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM) and differential scanning calorimetry (DSC) was carried out on the structure, surface morphology and thermal behaviour of the MA Al-Ti mixtures, both of milled and heat treated powders.
12 August 2019 in Metals and Materials International
1 July 2018 in Key Engineering Materials
ECEduardo Sanchez Caballero
Eduardo Sanchez Caballero
In order to produce metal matrix composites (MMCs), aluminium powder was milled for a total time of 5 hours. Aluminium nitride was the ceramic reinforcement chosen to improve the mechanical behaviour of the aluminium matrix. In order to form it in situ, an ammonia gas flow was incorporated during a certain period of the milling process. Two different conditions of NH3 flow during milling were studied: short time (5 min) and long time (3 h). In both cases, milling started with a 2 h period of mechanical alloy in vacuum (5 Pa). Then, NH3 was incorporated during the stipulated time (5 min or 3 h), after which the milling process continued under vacuum to complete 5 hours. The powders were cold pressed and vacuum sintered to produce compacts. The results showed that compacts with better mechanical properties are obtained when short duration ammonia gas flow is used. The use of short flows provides good control of the amount of ceramic second phases formed. This allows the produced compacts to reach ultimate tensile strength higher than 400 MPa.