Yitai Li

Yitai Li

Auto-generated profile, based on publicly available information

Yitai Li

School of Resources, Environment and Materials, Guangxi University, Nanning 530004, China

Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
11 April 2019 in Materials
Verified
Journal Article
Open access
PDF file
WYWenchao Yang
Wenchao Yang
JLJidong Li
Jidong Li
YLYitai Li
Yitai Li
JFJunli Feng
Junli Feng
JWJingwu Wu
Jingwu Wu
YZYongzhong Zhan
Yongzhong Zhan
This study investigates the effect of aluminum (Al) on the microstructure, micro-hardness, and wettability of environmentally friendly Sn-20Bi-xAl (x = 0, 0.1, 0.3, 0.5 (wt.%)) solder alloys. Scanning electron microscopy (SEM) with energy dispersive spectroscopy (EDS) analysis, and X-ray diffraction (XRD), were used to identify the microstructure morphology and composition. The spreading area and contact angle of the Sn-20Bi-xAl alloys on Cu substrates were used to measure the wettability of solder alloys. The results indicate that Al increased the hardness to a maximum value of ~27.1 HV for x = 0.5. When the content of Al was more than 0.3 wt.%, the hardness change value gradually flattened. From the spreading test results, Al reduced the wettability of solder alloys. When the content of Al was 0.1 wt.%, the change was slight. When more than 0.3 wt.%, the wettability of Sn-20Bi-xAl solder alloys sharply dropped. The corrosion resistance of Sn-20Bi-0.1Al alloy was the best, and the corrosion rate was at the lowest value at 0.092 mm/a due to the dense corrosion products.

28 July 2020 in Journal of Materials Science: Materials in Electronics
Verified
Journal Article
Closed access
PDF file
WYWenchao Yang
Wenchao Yang
YLYang Lv
Yang Lv
XZXinjiang Zhang
Xinjiang Zhang
XWXuanchen Wei
Xuanchen Wei
YLYitai Li
Yitai Li
YZYongzhong Zhan
Yongzhong Zhan

12 November 2019 in Materials
Verified
Journal Article
Open access
PDF file
WYWenchao Yang
Wenchao Yang
ZDZaixiang Du
Zaixiang Du
SYShuyuan Yu
Shuyuan Yu
YLYitai Li
Yitai Li
JFJunli Feng
Junli Feng
YZYongzhong Zhan
Yongzhong Zhan
Sn-0.7Cu-0.075Al solder alloy adding with Ce and La had been successfully prepared by applying ball-milling and vacuum arc remelting. The influence of Ce and La on microstructure and corrosion behavior of Sn-0.7Cu-0.075Al solder alloy was investigated. The results showed that Ce (La)-containing solders had refined grains and obvious directional tendency due to the dispersive refiner (CeO2 and La2O3). Electrochemical potentiodynamic curves revealed three different stages of the reaction, including anodic and cathodic processes, prepassivation section, and stable passivation stages. The self-corrosion potential (Ecorr) of alloys with Ce and La addition were a little bit more negative, hardly making a difference on corrosion occurrence. However, the corrosion current density (Icorr) and passivation current density (Ip) decreased by two-thirds and one-half respectively, which indicated a better corrosion resistant after adding rare earths. The recorded micrographs of corroded surface at different polarized points witnessed the formation of corrosion product film both on prepassivation and passivation stage. Moreover, the cross section of corrosion product film showed the coarse, loose film in Sn-0.7Cu-0.075Al solder and adherent, compact film in Ce (La)-containing solders, which further indicated an excellent anti-corrosion property.

28 June 2021 in Materials
Verified
Journal Article
Open access
PDF file
YLYitai Li
Yitai Li
WQWeiou Qin
Weiou Qin
SYShuyuan Yu
Shuyuan Yu
JLJun La
Jun La
YFYaokun Fu
Yaokun Fu
YZYongzhong Zhan
Yongzhong Zhan
The influences of non-isothermal aging (the temperature range is 150–180 °C, and the heating rate is 5 and 20 °C/h alternately), single-peak aging (aging at 120 °C for 24 h, then water quenched was followed at room temperature), and two-stage aging (aging at 105 °C for 8 h first, then increasing aging temperature to 135 °C and keeping for 12 h, followed by water quenching at room temperature) on the corrosion resistance and microstructure of the 7N01 aluminum alloy under 3.5 wt.% NaCl were investigated using electric polarization curve test and exfoliation corrosion. After aging, the hardness of samples was measured by a Vickers micro-hardness tester, and the electrical conductivities were obtained using the eddy current method. The results show that the steady phase η and metastable phase η′ are precipitated in the grain boundary of 7N01 aluminum alloy after non-isothermal aging, and their distribution is discontinuous. The hardness of the alloy can reach 136.9 HV1 and the electrical conductivity can reach 35.8% IACS, which is close to the hardness of single-peak aging and the conductivity of two-stage aging, respectively. Compared with single-peak aging, the corrosion current density of non-isothermal aging is reduced by 15.5%, and that of two-stage aging is reduced by 28.9%.

28 January 2022 in Journal of Materials Science: Materials in Electronics
Verified
Journal Article
Closed access
PDF file
QSQianqian Song
Qianqian Song
YLYitai Li
Yitai Li
JYJinli Yu
Jinli Yu
DQDa Qi
Da Qi
WQWeiou Qin
Weiou Qin
YZYongzhong Zhan
Yongzhong Zhan