6 September 2018 in Scientific Reports
Perpendicular magnetic materials with low damping constant and high thermal stability have great potential for realizing high-density, non-volatile, and low-power consumption spintronic devices, which can sustain operation reliability for high processing temperatures. In this work, we study the Gilbert damping constant (α) of perpendicularly magnetized W/CoFeB/MgO films with a high perpendicular magnetic anisotropy (PMA) and superb thermal stability. The α of these PMA films annealed at different temperatures (Tann) is determined via an all-optical Time-Resolved Magneto-Optical Kerr Effect method. We find that α of these W/CoFeB/MgO PMA films decreases with increasing Tann, reaches a minimum of α = 0.015 at Tann = 350 °C, and then increases to 0.020 after post-annealing at 400 °C. The minimum α observed at 350 °C is rationalized by two competing effects as Tann becomes higher: the enhanced crystallization of CoFeB and dead-layer growth occurring at the two interfaces of the CoFeB layer. We further demonstrate that α of the 400 °C-annealed W/CoFeB/MgO film is comparable to that of a reference Ta/CoFeB/MgO PMA film annealed at 300 °C, justifying the enhanced thermal stability of the W-seeded CoFeB films.
2 September 2020 in Physical Review B
Strain-free thin films were obtained on MgO (001) single-crystal substrates with Cr seed layers. X-ray diffraction and transmission electron microscopy confirmed that the film is textured in all three spatial directions with crystallographic orientation determined by epitaxial constraints from the substrate. Average grain size was estimated to be in the range of tens of nanometers. Ten pieces of 40-nm-thick thin-film samples were stacked together for half-polarized neutron diffraction study at room temperature. A total of six reflections were usable, from which the magnetic structure of was determined and compared to existing models. Contrary to most electronic structure calculations, the present results suggest that the magnetic moment of Fe atoms at the site is large and larger than that of the site. Our results support the giant magnetization of .
7 May 2018 in Applied Physics Letters
Metastable -Fe16N2 has attracted much interest as a candidate for rare-earth-free hard magnetic materials. We demonstrate that Fe16N2 thin films were grown epitaxially on Cr seed layers with MgO (001) substrates by facing-target sputtering. Good crystallinity with the epitaxial relation was obtained. The chemical order parameter, which quantifies the degree of N ordering in the Fe16N2 (the N-disordered phase is -Fe8N martensite), reaches 0.75 for Cr-seeded samples. Cr has a perfect lattice constant match with Fe16N2, and no noticeable strain can be assigned to Fe16N2. The intrinsic saturation magnetization of this non-strained Fe16N2 thin film at room temperature is determined to be 2.31 T by polarized neutron reflectometry and confirmed with vibrating sample magnetometry. Our work provides a platform to directly study the magnetic properties of high purity Fe16N2 films with a high order parameter.
3 January 2020 in Journal of Magnetism and Magnetic Materials
1 November 2019 in Journal of Physics D: Applied Physics
The exchange coupling effect in nanocomposite samples with ferromagnetic (FM) body-centred tetragonal (bct) Fe nanoparticles (NPs) (~20 nm) embedded in an MnN antiferromagnetic (AFM) matrix is investigated. Both the bct Fe NPs control sample and the MnN (×nm)\bct Fe NPs\MnN (20–35 nm)\Ta (5 nm) nanocomposite samples are synthesized by a gas-phase condensation method. Both the coercivity and the remanence ratio of the nanocomposite samples are significantly enhanced compared with the bct Fe NPs sample. The coercivity and the remanence ratio increase with MnN thickness up to 30 nm and then decrease. Additionally, the exchange coupling strength between the bct Fe NPs and AFM MnN matrix is enhanced by magnetic field training. The magnetic field training leads to a higher coercivity and remanence ratio after one cycle of field-cooled hysteresis loop measurement. The coercivity of the composite sample increases by 80%, while the remanence ratio increases by around 30% compared with the bct Fe NPs sample. This work may provide an alternative approach to the design and manufacturing of FM-AFM exchange-coupled permanent magnets.
24 August 2026 in Journal of Magnetism and Magnetic Materials