Well-aligned ZnO nanowire arrays with a long length of more than 40 microm were prepared successfully by using the polyethylenimine (PEI)-assisted preheating hydrothermal method (PAPHT). Several important synthetic parameters such as PEI content, growth time, preheating time and zinc salt concentration were found to determine the growth of ultralong ZnO nanowire arrays, including length, diameter, density and alignment degree. The photoluminescence (PL) spectrum of as-grown ultralong ZnO nanowire arrays revealed a UV emission and a yellow emission, which was attributed to the absorbed hydroxyl group based on the peak shift after annealing in various atmospheres. The performance of dye-sensitized solar cells (DSSCs) increased with increasing length of ZnO nanowire arrays, which was mainly ascribed to the aggrandized photocurrent and reduced recombination loss according to electrochemical impedance spectroscopy (EIS). A maximum efficiency of 1.3% for a cell with a short-circuit current density (J(sc)) = 4.26 mA cm(2), open-circuit voltage (V(oc)) = 0.69 V and (fill factor) FF = 0.42 was achieved with a length of 40 microm.
The synthesis of ZnO nanostructures via the transformation strategy from zinc-based compounds has long been hampered by the difficulties in obtaining high quality nanostructures. Herein we report a simple and effective method toward nanocrystalline/nanoporous ZnO nanostructures with well-defined shapes transformed from zinc fluorohydroxide Zn(OH)F deposited on Si substrate. The traditional reaction route of zinc chloride-hexamethylenetetramine system toward ZnO was deviated by the use of fluorion (F−) additive through a simple solvothermal process in H2O–ethanol component solvent, resulting in the formation of Zn(OH)F crystals. Three kinds of micron shape (sphere, hexapod and hexagonal disk) and two kinds of microstructure (nanocrystalline and nanoporous) were demonstrated, merely by varying the concentration of F− ions and the sintering temperature. While the concentration of F− ions directly determined the phase and morphology of the as-deposited nanostructures, the ultra smooth nature of the Si substrate and the component solvent affected significantly the nucleation, the self-assembly behavior and the crystallinity of each Zn(OH)F prism. The formation mechanism of Zn(OH)F hexapod was discussed from two points, the Si-controlled nucleation on already-formed particles, and the [F−]-dependent crystallization process. Furthermore, the self-assembly of multiple Zn(OH)F/ZnO disks and the selective growth of Zn(OH)F hexapods was demonstrated by reducing the growth rate and by inducing the nucleation on the patterned gold layer, respectively.
A single-crystalline twinned ZnO nanostructure with a 2-dimensional leaf-like morphology (nanoleaves) was synthesized using a facile hydrothermal strategy. The ZnO nanoleaves had 2-fold symmetric branches, which were identified by the existence of an inversion domain boundary (IDB) along the [2110] growth direction of the ribbon-like stems with both side surfaces of the stems terminated with a chemically active Zn-(0001) plane. A proposed growth mechanism suggested that the formation of IDB and the leaf-like shape are related to the dissolution of seed particles on the substrate surfaces and an OH− shielding effect in solution, respectively. Optical measurements revealed visible emission, suggesting the possession of defects in the as-grown and annealed ZnO nanoleaves. In addition, various ZnO nanostructures were synthesized by simply controlling the fabrication conditions.