Tungsten oxide–silicon dioxide (WOx–SiOy) composite thin films were deposited for the first time via the remote oxygen plasma-enhanced atomic layer deposition (ALD) process using a novel metal-organic heteronuclear and heteroleptic precursor, bis(tert-butylimido)bis(trimethylsilylmethyl)tungsten. Self-limiting ALD growth was demonstrated over a wide temperature window of 203–328 °C with growth per cycle decreasing with increasing temperature from 0.75 to 0.4 Å/cycle, respectively. Residual gas analysis revealed ligand competition and showed that ligand reaction during ALD nucleation and growth was a function of deposition temperature, thereby affecting the film composition. As the temperature increased from 203 to 328 °C, the film composition [W/(Si + W)] ranged from 0.45 to 0.53. In addition, the carbon impurity content was reduced and the refractive index increased from 1.73 to 1.96, the density increased from 4.63 to 5.6 g/cm3, and the optical bandgap decreased from 3.45 to 3.27 eV. Grazing angle x-ray diffraction indicated that as-deposited films were amorphous. Upon annealing in O2 at 500 °C or higher, depending on deposition temperature, films are crystalized into the triclinic WO3 phase. At the same time, WO3 is sublimed from the surface and films are reduced in thickness.
Ferroelectric tunnel junctions (FTJs) utilizing hafnium zirconium oxide (HZO) have attracted interest as non-volatile memory for microelectronics due to ease of integration into back-end-of-line (BEOL) complementary metal oxide semiconductor fabrication. This work examines asymmetric electrode NbN/HZO/Nb devices with 7 nm thick HZO as FTJs in a memory structure, with an output resistance that can be controlled by read and write voltages. The individual FTJs are measured to have a tunneling electroresistance of 10 during the read state without significant filament conduction formation and reasonable ferroelectric performance. Endurance and remanent polarizations of up to 105 cycles and 20 μC/cm2, respectively, are measured and are shown to be dependent on the cycling voltage. Electrical measurements demonstrate how magnitude of the write pulse can modulate the high state resistance and the read pulse influences both resistance values as well as separation of resistance states. Then, by using two opposite switching FTJ devices in series, a programmable nonvolatile resistor divider is demonstrated. Measurements of these two FTJ unit memory cells show wide applicability to a BEOL microfabrication process for a re-readable, rewritable, and nonvolatile memory cell.
Self-limiting, purge-separated, cyclic reactions enable atomic layer deposition (ALD) to produce highly uniform and conformal films with precise thickness control. However, the typical relatively low deposition temperatures can lead to residual impurities, defects, and suboptimal material properties. To address this, we introduce microwave enhanced ALD (MW-ALD), an energy enhanced ALD technique in which in situ microwave exposure is included in each ALD cycle. The design of the microwave antenna and exposure system and integration into a commercial ALD chamber are first described. The benefits of MW-ALD are then demonstrated using Al2O3, a material that in bulk form is not expected to strongly interact with microwaves. Through ellipsometry and electrical measurements, we show that in situ MW irradiation annealing can reduce thickness, improve film properties such as refractive index, reduce high field current leakage, and improve breakdown strength. In all cases, MW-ALD produced a greater change in properties than was produced by an equivalent microwave exposure performed post deposition.
Metal/insulator interfaces impact the performance of electron devices through a variety of process dependent extrinsic effects. Bilayer-metal electrodes employing a reactive interfacial metal are often used to promote the adhesion of an overlying inert cap metal to an oxide. Bilayer-metal stacks have been proposed to decouple the influence of some extrinsic effects, such as interfacial defects from others such as strain and metal grain size, to assist in the optimization of silicon quantum bits. In this work, we used internal photoemission spectroscopy to directly measure the influence of the interfacial Ti thickness on the electron energy barrier at the Pt/Ti/Al2O3 bilayer-metal/insulator interface of Pt/Ti/Al2O3/TiN devices. We found that a 0.5 to 1.0 nm thick layer of Ti was sufficient to completely dominate the electron energy barrier. Insertion of a Ti layer also resulted in band tailing, likely due to oxygen scavenging, but had no impact on the bottom Al2O3/TiN electrode barrier.