9 January 2025 in Materials
Verified
Journal Article
Open access
PDF file
JCJinhua Cao
Jinhua Cao
SWShuaihu Wei
Shuaihu Wei
XWXiaoming Wang
Xiaoming Wang
XLXuejian Li
Xuejian Li
MLMuyuan Li
Muyuan Li
Xiaojun WangXiaojun Wang
Xiaojun Wang
Grain refinement is of very important significance for improving the microstructure and mechanical properties of Mg alloys. This work investigated how the addition of various amounts of Y element affected the microstructure and mechanical properties of Mg-9Al-1Zn alloy. It was found that the grain size of Mg-9Al-1Zn alloy decreases as Y element content increases. When 1.2 wt.% Y element content was added, the grain size of Mg-9Al-1Zn alloy could be reduced from 334.2 μm to 134.6 μm, and grain refinement efficiency of 60% was achieved. HRTEM analysis demonstrated a good orientation relationship between the Al2Y phase and the Mg interface, and therefore, it was determined that the Al2Y phase can be used as a heterogeneous nucleation site for α-Mg grains, which promotes the grain refinement of α-Mg grain. Furthermore, the addition of Y element can also significantly refine the eutectic Mg17Al12 phase of the Mg-9Al-1Zn alloy. In this way, the mechanical properties of the Mg-9Al-1Zn alloy are significantly enhanced. It was found that the YS and UTS of the Mg-9Al-1Zn alloy reached 87 MPa and 154 MPa with the addition of 0.9 wt.% of Y element—24% and 43% higher than the Mg-9Al-1Zn alloy.

14 October 2026 in Metals
Verified
Journal Article
Open access
PDF file
XWXiaoming Wang
Xiaoming Wang
JWJinhui Wang
Jinhui Wang
TMTong Mu
Tong Mu
JCJingya Cui
Jingya Cui
HLHonghui Liu
Honghui Liu
YZYongcai Zhang
Yongcai Zhang
Mg-Nd-Gd-Zn-Zr alloys containing 0, 0.20, and 0.75 wt.% Sr were prepared by gravity casting to investigate the effects of Sr microalloying on as-cast microstructure, solution-treatment response, and age-hardening behavior. The alloys were characterized by XRD, OM, SEM/EDS, DSC, and Brinell hardness testing. Sr was mainly enriched at grain boundaries and in secondary-phase regions, and Mg17Sr2-related diffraction peaks appeared in the Sr-containing alloys. The as-cast grain size varied non-monotonically among the three compositions investigated, with the 0.20 wt.% Sr alloy exhibiting the finest grains, whereas the area fraction of secondary phases increased continuously with Sr content. Under the selected solution-treatment conditions, the Sr-containing alloys retained smaller grains but contained larger amounts of residual secondary phases. Under the respective selected solution-treated starting states, the 0Sr alloy achieved the highest measured hardness at 200 °C, while the 0.20Sr alloy showed an earlier hardening response and a more gradual subsequent hardness evolution; the 0.75Sr alloy showed a more pronounced post-peak hardness decrease. The retained Sr-containing secondary phases may indicate incomplete dissolution of part of the Nd, Gd, and Zn, potentially reducing the effective solute reservoir in α-Mg available for subsequent aging. Within the three compositions investigated, the results indicate a trade-off between grain refinement/retention and age-hardening potential.