The dependence of the catalytic activity and coke resistance of Ni-based catalysts on the support type was investigated in the dry reforming of methane (DRM). Catalysts were prepared using incipient wetness impregnation and analyzed using ICP-OES, BET-BJH, XRD, H2-chemisorption, H2-TPR, and CO2-TPD. DRM was performed at 600–750 °C at 144,000 mL/gcat∙h of GHSV (CH4/CO2/N2 = 1/1/1). Ni/Al2O3 and Ni/MgO catalysts formed NiAl2O4 and NiO-MgO solid solutions, respectively, owing to strong binding between the metal and support. In contrast, MgO-Al2O3 and MgAl2O4 supports suppressed NiAl2O4 and NiO-MgO solid solution formation, due to Mg addition, with high metal dispersions of 4.6 and 6.6%, respectively. In the DRM reaction, the Ni/MgO-Al2O3 and Ni/MgAl2O4 catalysts showed high CH4 conversions of 78.1 and 76.8%, respectively, compared with Ni/Al2O3 and Ni/MgO at 750 °C. A stability test was performed at 600 °C for 20 h. A coke study of the spent catalysts was performed using SEM and TGA. Alkaline-earth metal-containing catalysts Ni/MgO-Al2O3 and Ni/MgAl2O4 with strong CO2 adsorption properties showed 20 wt% reduction in carbon deposition compared to commercial catalysts. Therefore, the support and basic properties of the catalyst significantly influenced the catalyst performance and coke resistance in the DRM.
25 November 2022 in Journal of Industrial and Engineering Chemistry
A small loading of highly dispersed Ru on Ni/MgAl2O4 catalyst was investigated in the dry reforming of methane (DRM) process. The catalysts were synthesized by impregnation and deposition-precipitation methods; the DRM reaction was performed at CH4/CO2/N2 = 1/1/1 and 600‒750°C. The bimetallic Ni‒Ru catalysts exhibited improved reducibility and metal dispersion compared with that of the Ni catalyst. Among the synthesized catalysts, the Ru(D)/Ni(I)/MgAl2O4 catalyst had the highest metal dispersion (7.23%) and largest amount of CO2 desorption (135 μmol/g). Thus, this catalyst exhibited the highest CH4 conversion (85.6%) at 750°C. Additionally, coke deposition of only 2.69% occurred during the stability test.