Solid‐state batteries are considered as a reasonable further development of lithium‐ion batteries with liquid electrolytes. While expectations are high, there are still open questions concerning the choice of materials, and the resulting concepts for components and full cells. On the basis of an analysis of all materials and concept options, a roadmap for solid‐state batteries is presented, relying on both literature survey and experts' opinions. Diverse cell concepts with different solid electrolytes may be developed up to the commercial level, yet there are still major uncertainties concerning production routes, safety as well as cost. As one of the key developments, it appears that hybrid material and cell concepts may be particularly successful on the way to commercialization.
4 July 2022 in Angewandte Chemie International Edition
We present the convenient synthesis and characterization of the new ternary thiostannate Na4SnS4 (space group ) by directed removal of crystal water molecules from Na4SnS4⋅14 H2O. The compound represents a new kinetically stable polymorph of Na4SnS4, which is transformed into the known, thermodynamically stable form (space group ) at elevated temperatures. Thermal co‐decomposition of mixtures with Na3SbS4⋅9 H2O generates solid solution products Na4−xSn1−xSbxS4 (x=0.01, 0.10) isostructural to the new polymorph (x=0). Incorporation of Sb5+ affects the bonding and local structural situation noticeably evidenced by X‐ray diffraction, 119Sn and 23Na NMR, and 119Sn Mössbauer spectroscopy. Electrochemical impedance spectroscopy demonstrates an enormous improvement of the ionic conductivity with increasing Sb content for the solid solution (σ25°C=2×10−3, 2×10−2, and 0.1 mS cm−1 for x=0, 0.01, and 0.10), being several orders of magnitude higher than for the known Na4SnS4 polymorph.
The Na storage mechanism of Fe3S4 nanoparticles is studied via electrochemical techniques, synchrotron-based X-ray diffraction and absorption methods. The results explain the relation of the electrodes cycle life and cut-off potentials.
15 August 2022 in Journal of Solid State Electrochemistry
We present new insights into the electrochemical properties of three metal sulfides MCr2S4 (M = Cr, Ti, Fe) probed as anode materials in sodium-ion batteries for the first time. The electrodes deliver decent reversible capacities and good long-term cycle stability, e.g., 470, 375, and 524 mAh g−1 are obtained after 200 cycles applying 0.5 A g−1 for M = Cr, Ti, and Fe, respectively. The reaction mechanisms are investigated via synchrotron-based X-ray powder diffraction and pair distribution function analyses. The highly crystalline educts are decomposed into Na2S nanoparticles and ultra-small metal particles during initial discharge without formation of intermediate NaCrS2 domains as previously reported for CuCrS2 and NiCr2S4. After a full cycle, the structural integrity of MCr2S4 (M = Cr, Ti, Fe) is not recovered. Thus, the Na storage properties are attributed to redox reactions between nanoscopic to X-ray amorphous conversion products with only local atomic correlations M···S/S···S in the charged and M···M/Na···S in the discharged state. Graphical Abstract
27 January 2023 in European Journal of Inorganic Chemistry
The new thiostannate Na4Sn2S6 was prepared by directed crystal water removal from the hydrate Na4Sn2S6 ⋅ 5H2O at moderate temperatures. While the structure of the hydrate comprises isolated [Sn2S6]4− anions, that of the anhydrate contains linear chains composed of corner‐sharing SnS4 tetrahedra, a structural motif not known in thiostannate chemistry. This structural rearrangement requires bond‐breakage in the [Sn2S6]4− anion, movements of the fragments of the opened [Sn2S6]4− anion and Sn−S−Sn bond formation. Simultaneously, the coordination environment of the Na+ cations is significantly altered and the in situ formed NaS5 polyhedra are joined by corner‐ and edge‐sharing to form a six‐membered ring. Time‐dependent in situ X‐ray powder diffraction evidences very fast rehydration into Na4Sn2S6 ⋅ 5H2O during storage in air atmosphere, but recovery of the initial crystallinity requires several days. Impedance spectroscopy demonstrates a mediocre room‐temperature Na+ ion conductivity of 0.31 μS cm−1 and an activation energy for ionic transport of Ea=0.75 eV.
16 November 2022 in Chemistry – A European Journal
A highly unusual solid‐state epitaxy‐induced phase transformation of Na4SnS4 ⋅ 14H2O (I) into Na4Sn2S6 ⋅ 5H2O (II) occurs at room temperature. Ab initio molecular dynamics (AIMD) simulations indicate an internal acid‐base reaction to form [SnS3SH]3−which condensates to [Sn2S6]4−. The reaction involves a complex sequence of O−H bond cleavage, S2−protonation, Sn−S bond formation and diffusion of various species while preserving the crystal morphology. In situ Raman and IR spectroscopy evidence the formation of [Sn2S6]4−. DFT calculations allowed assignment of all bands appearing during the transformation. X‐ray diffraction and in situ1H NMR demonstrate a transformation within several days and yield a reaction turnover of ≈0.38 %/h. AIMD and experimental ionic conductivity data closely follow a Vogel‐Fulcher‐Tammann typeTdependence withD(Na)=6×10−14 m2 s−1atT=300 K with values increasing by three orders of magnitude from −20 to +25 °C.