1 December 2013 in Materials Characterization
1 March 2016 in Materials Characterization
2 July 2015 in Key Engineering Materials
Advanced high strength steel (AHSS) was prepared using the conventional ‘press and sinter’ process.The compacts of ultralow carbon Fe-Cr-Mo powder with carbon additions (base metal powder admixed with 0.1,0.2 and 0.3 wt.% graphite) and without carbon addition (plain base powder) were sintered in a vacuum furnace at pressure of 1.28 x 10-5MPa at 1280 °C for 45 min. After sintering, the sintered specimens were continuously cooled with different nitrogen gas pressures of 0, 2500 and 5000 mbars (or 0, 0.25, 0.5 MPa). Mechanical properties of the sintered alloys were strongly controlled by carbon contents and cooling rates after sintering. The sintered specimens, with 0.3 wt.% carbon and cooled by nitrogen of 5000 mbars, showing superior tensile strengths and good ductility, had microstructures dominated by carbide-free bainitic structures and some retained austenite. The sintered specimens with lower carbon contents and cooled under slower cooling rates, having lower tensile strengths but slightly higher ductility, had microstructures with lower bainite volume fractions and even without bainitic structures. The dominant phase in the sintered specimens with low strength but high ductility was ferrite.
1 May 2021 in IOP Conference Series: Materials Science and Engineering
The use of pre-alloyed Fe-Cr based powders has been steadily increasing in the automotive industry. Mechanical properties can be tailored due to phase transformations controlled by alloying elements and cooling rates. Employing silicon carbide (SiC) as a source of alloying elements has been proved to be possible. In this study, three different pre-alloyed Fe-Cr based powders, namely Astaloy CrA, Astaloy CrL, and Astaloy CrM, were alloyed with 4 wt. % SiC powder. The powders were mixed and pressed into tensile test bars. The green compacts were sintered at 1250 °C for 45 minutes under the cracked ammonia gas and slowly cooled (<0.1°C/s) to room temperature. All experimental sintered alloys manifested a common feature resembling those of full pearlitic ductile irons, i.e., the feature consisted of black nodular particles enveloped with hyper-eutectoid steel matrix (grain boundary or pro-eutectoid cementite plus pearlite). The tensile testing indicated that Alloy-3 (Astaloy CrM + 4%SiC) was observed to have better mechanical properties in comparison with Alloy-1 (Astaloy CrA + 4%SiC) and Alloy-2 (Astaloy CrL + 4%SiC), apart from slightly lower elongation than Alloy-2. Regardless of SiC addition, the presence of chromium (Cr) content was observed to substantially influence mechanical properties and microstructure. According to the investigation of fracture surfaces by SEM, mixtures of shallow dimples and cleavage fractures were examined in the sintered alloys.
15 October 2024 in ISIJ International
This work demonstrated that the silicon carbide addition to pre-alloyed Fe-Mo powder could result either in the formation of steel or iron microstructure depending on the added silicon carbide content. With 1.0 wt. % silicon carbide addition, slowly cooled sintered Fe-Mo-Si-C alloys showed steel microstructures consisting of proeutectoid ferrite and eutectoid transformation product in the form of ferrite + carbide mixture. With 2.0 wt. % silicon carbide addition, slowly cooled sintered Fe-Mo-Si-C alloys with Mo contents of ≥ 0.85 wt.% microstructures comprised ferrite + austenite constituents in the forms of either degenerate upper bainite or ausferrite. With ≥ 3.0 wt. % silicon carbide addition, ductile iron-like microstructures were developed in sintered Fe-Mo-Si-C alloys. The change of microstructures in experimental sintered alloys was attributed to the combined effect of alloying molybdenum, silicon, and carbon elements. Tensile strength and hardness increased with increasing added SiC content while ductility varied with microstructural components.