Pongsak Wila

Pongsak Wila

Auto-generated profile, based on publicly available information

Pongsak Wila

National Metal and Materials Technology Center (MTEC)

Research Focus & Metrics

Academic Career Length

14Years (2013-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 December 2013 in Materials Characterization
Verified
Journal Article
Closed access
RTRuangdaj Tongsri
Ruangdaj Tongsri
TYThanyaporn Yotkaew
Thanyaporn Yotkaew
RKRungtip Krataitong
Rungtip Krataitong
PWPongsak Wila
Pongsak Wila
ASAutcharaporn Sir-On
Autcharaporn Sir-On
NTNattaya Tosangthum
Nattaya Tosangthum

1 January 2018 in Materials Today: Proceedings
Verified
Journal Article
Closed access
NTNattaya Tosangthum
Nattaya Tosangthum
MMMonnapas Morakotjinda
Monnapas Morakotjinda
RKRungtip Krataitong
Rungtip Krataitong
PWPongsak Wila
Pongsak Wila
TYThanyaporn Yodkaew
Thanyaporn Yodkaew
RTRuangdaj Tongsri
Ruangdaj Tongsri

2 April 2019 in Key Engineering Materials
Verified
Journal Article
Closed access
PDF file
NTNattaya Tosangthum
Nattaya Tosangthum
PKPrapas Kunnam
Prapas Kunnam
MMMonnapas Morakotjinda
Monnapas Morakotjinda
WKWantana Koetniyom
Wantana Koetniyom
RKRungtip Krataitong
Rungtip Krataitong
RTRuangdaj Tongsri
Ruangdaj Tongsri
Sintered steels, with and without boron addition, were prepared from powder compacts of pre-alloyed Fe-1.5Mo powder mixed with varied amounts of graphite (0, 0.1, 0.2, 0.3, and 0.4 wt.%) and hexagonal boron nitride (0 and 0.5 wt.%). Sintering was performed either in hydrogen or in vacuum atmosphere at 1280 °C for 45 minutes. The post-sintering cooling was performed in a furnace that was equivalent to 0.1 °C/s. The sintered boron-free steels showed dual-phase microstructure consisting polygonal ferrite and precipitate-containing grains. Each precipitate-containing grain contained packets, each of which was characterized by lamellar structure with alternating fibrous particles and ferritic laths, when carbon contents were in the range 0.1-0.3 wt.%. All the grains containing fine needle particles decorating ferritic lath boundaries were observed in the sintered Fe-Mo-0.4C steels. Boron addition caused some effects on sintered steels. The action of boron was the formation of grain boundary boride in the vacuum-sintered steels although it was hardly observed in case of hydrogen-sintered steels. Boron also promoted precipitation inside polygonal ferrite grains and along ferritic lath boundaries. The precipitate particle shape was fine needle-like in the sintered boron-containing steels. Due to liquid phase sintering, as a result of eutectic melting, the associated grain growth was observed. Disappearance of grain boundary boride was evidenced in the hydrogen-sintered steels. Without boron addition, hardening of the sintered steels strongly depended on carbon content. With boron addition, all the sintered steels showed high tensile strength and hardness even in the case of no graphite addition. Hardening action by carbon in the sintered boron-containing steels was weaker than that in the sintered boron-free steels.

1 May 2021 in IOP Conference Series: Materials Science and Engineering
Verified
Conference Paper
Open access
ASA.N. Soe
A.N. Soe
PWP. Wila
P. Wila
MMM. Morakotjinda
M. Morakotjinda
TYT. Yotkaew
T. Yotkaew
PKPreechar Karin
Preechar Karin
RTRuangdaj Tongsri
Ruangdaj Tongsri
The use of pre-alloyed Fe-Cr based powders has been steadily increasing in the automotive industry. Mechanical properties can be tailored due to phase transformations controlled by alloying elements and cooling rates. Employing silicon carbide (SiC) as a source of alloying elements has been proved to be possible. In this study, three different pre-alloyed Fe-Cr based powders, namely Astaloy CrA, Astaloy CrL, and Astaloy CrM, were alloyed with 4 wt. % SiC powder. The powders were mixed and pressed into tensile test bars. The green compacts were sintered at 1250 °C for 45 minutes under the cracked ammonia gas and slowly cooled (<0.1°C/s) to room temperature. All experimental sintered alloys manifested a common feature resembling those of full pearlitic ductile irons, i.e., the feature consisted of black nodular particles enveloped with hyper-eutectoid steel matrix (grain boundary or pro-eutectoid cementite plus pearlite). The tensile testing indicated that Alloy-3 (Astaloy CrM + 4%SiC) was observed to have better mechanical properties in comparison with Alloy-1 (Astaloy CrA + 4%SiC) and Alloy-2 (Astaloy CrL + 4%SiC), apart from slightly lower elongation than Alloy-2. Regardless of SiC addition, the presence of chromium (Cr) content was observed to substantially influence mechanical properties and microstructure. According to the investigation of fracture surfaces by SEM, mixtures of shallow dimples and cleavage fractures were examined in the sintered alloys.

22 August 2017 in Key Engineering Materials
Verified
Journal Article
Closed access
PDF file
ASAmnart Suksamran
Amnart Suksamran
NWNawarat Worauaychai
Nawarat Worauaychai
NTNattaya Tosangthum
Nattaya Tosangthum
TYThanyaporn Yodkaew
Thanyaporn Yodkaew
RKRungtip Krataitong
Rungtip Krataitong
RTRuangdaj Tongsri
Ruangdaj Tongsri
Five multi-component alloy (MCA) formulations of CoFeMnNiZn (MCA01), Al0.5CoFeMnNiZn (MCA02), Al1.0CoFeMnNiZn (MCA03), Co5Fe5Mn30Ni20Zn40 (MCA04) and Al8.4Co4.6Fe4.6Mn27Ni18.4Zn37 (MCA05) were prepared by mechanical alloying and melting process (MAM). Five-component alloys of MCA01-MCA05 were designed using empirical formulae for high entropy alloys. Phase formation and microstructure were evaluated by X-ray diffraction (XRD) and scanning electron microscopy (SEM). The results showed that MCA01 was partially melted by MAM process. However, MCA02-MCA05 could be melted and cast by MAM process. The microstructures of as-cast MCA02 and MCA03 showed dendritic solidification. Nevertheless, the as-cast MCA04 showed microstructure similar to that of Ni-based superalloy, i.e., the as-cast MCA04 consisted of γ matrix and γ′ phase. Moreover, egg type core shell structure was found in the interdendritic regions of the MCA05 alloy. In addition, the Al-added MCA02 and MCA03 alloys showed crystal structures of FCC1, FCC2 and BCC. MCA04 alloy demonstrated crystal structure of FCC whereas MCA05 alloy had crystal structures of FCC and Primitive Cubic.