In this paper surface-alloyed layers formed on titanium VT1-0 substrates by non-vacuum electron beam cladding of Ta and Zr powder mixture are investigated. It has been found that the clad layers have a defect-free structure with a distinct dendritic segregation over the cross section of the layer. The tantalum and zirconium concentration in the clad layer is 17 wt. % and 20 wt. %, respectively. Electron beam cladding does not significantly reduce the fracture toughness of the “clad layer – titanium substrate” bimetallic composite; the value of fracture energy remained at a sufficiently high level of 172.9 J/cm2. The surface alloying of titanium with tantalum and zirconium allows the corrosion resistance of titanium in a boiling 5 % HCl solution to be increased 17.3 times.
This study is devoted to the titanium trialuminides (TiAl3) formation during non-vacuum electron beam cladding over titanium substrates. The microstructure of the obtained materials was studied using optical microscopy and scanning electron microscopy (SEM). The thickness of the coatings is approximately 2 mm. There are no considerable pores or delamination in the materials. The phase composition and the chemical composition were determined using synchrotron X-ray radiation diffraction and X-ray dispersive analysis, respectively. The average value of the components in the coatings is 30 at. % Ti, 61 at. % Al and 9 at. % Cr. It was found that there is an existence of primarily two titanium trialuminide phases – Ti25Al67Cr8 (cubic crystalline structure) and close to stoichiometric TiAl3 (tetragonal crystalline structure). Besides, particles of Cr are evenly distributed through the coatings. The mechanical properties were evaluated by Vicker’s hardness tests under different loads. It was estimated that the microhardness level of the coatings (550±30 HV) is 5-6 times higher than the microhardness of the base material (100 HV).