In this study, electrospun nanofibers of poly(vinylidene fluoride) (PVDF) were produced with the addition of [6,6]-phenyl-C61-butyric acid methyl ester (PCBM) and poly(3-hexylthiophene) (P3HT), for application as a nanostructured active layer of bulk heterojunction polymer with fullerene and polythiophene derivatives in third-generation photovoltaic devices. The electrospinning technique was used to favor the formation of the β phase, exhibiting ferroelectric properties, improving the electrical performance of the device. The morphological, structural and electrical characteristics of the nanofibers were investigated using scanning electron microscopy (SEM), Fourier transform infrared spectroscopy (FTIR) and DC electrical measurements. The synergism between nanofiber processing and the addition of P3HT and PCBM improved electrical conductivity by up to three orders of magnitude, furthermore, the nanofibers incorporating P3HT exhibited responses to solar stimuli.
Electrospun poly(methyl methacrylate)/polypyrrole (PMMA/PPy) nanofibrous mats were engineered as ammonia-vapor sensing materials by varying the PPy content from 0 to 16 wt.%. The effect of composition on fiber morphology, electrical transport, structural features, and sensing performance was systematically investigated. PPy addition reduced the mean fiber diameter from 1130 to 730 nm and increased electrical conductivity by more than five orders of magnitude, reaching 9.06 × 10−5 S m−1 at 8 wt.% PPy. FTIR confirmed successful PPy incorporation while preserving the characteristic PMMA structure. Under cyclic N2/NH3 exposure, the 4 wt.% PPy mat exhibited the largest relative resistance variation together with stable and reproducible cycling behavior, whereas further increases in PPy content reduced the response amplitude. These findings highlight electrospun PMMA/PPy mats as low-cost candidates for ammonia sensing.
Electrospun poly(vinylidene fluoride)/reduced graphene oxide (PVDF/rGO) nanofibers were developed to investigate the influence of rGO content on fiber morphology, crystalline structure, and ammonia sensing performance. PVDF and PVDF/rGO composites containing 2, 4, and 6 wt.% rGO were fabricated by electrospinning and characterized by scanning electron microscopy, Fourier transform infrared spectroscopy, and electrical measurements. The incorporation of rGO progressively reduced the average fiber diameter from 326 ± 122 nm for neat PVDF to 175 ± 46 nm for the sample containing 6 wt.% rGO, while preserving a high fraction of the electroactive β-phase in all compositions. The developed nanofibrous mats exhibited reproducible electrical responses under NH3 exposure, with the PVDF/6 wt.% rGO sample showing the highest current variation (approximately 120 nA) and the fastest response time (10 s), compared with 15 s for pure PVDF. The improved sensing performance is attributed to the combined effects of reduced fiber diameter, favorable morphological characteristics, and the increased availability of active sites provided by rGO. These findings demonstrate that controlling the rGO content is an effective strategy for tailoring the morphology and electrical response of electrospun PVDF nanofibers, highlighting the potential of the PVDF/rGO system as a promising platform for ammonia sensing applications.