In this work, the WC-NiCrBSi and in-situ synthesised WC (IWC)-NiCrBSi coatings were successfully fabricated on SS 316 L using vacuum cladding process to investigate the WC-reinforced NiCrBSi alloy by the two methods. XRD, SEM and EDS were performed to characterise the phase constituents, microstructure and chemical composition, respectively. Subsequently, electrochemical corrosion and cavitation tests of the coatings were carried out in 3.5 wt-% NaCl solution. The results showed that the WC-NiCrBSi cladding coating was mainly composed of γ-Ni, FeNi3, WC, Cr23C6 and CrB phases, while the IWC-NiCrBSi cladding coating was composed of γ-Ni, WC, FeNi3, Cr23C6, Cr7C3, CrB phases. The corrosion current density of the WC-NiCrBSi and IWC-NiCrBSi coatings were 5.01 × 10−7 and 3.57 × 10−7 A/cm2, respectively. The combined analysis of cumulative weight loss curve and cavitation morphology revealed a better cavitation resistance by the IWC-NiCrBSi coating than the WC-NiCrBSi coating in 3.5 wt-% NaCl solution.
Fe-based coatings with high V and Cr content were obtained by laser cladding using Fe-based powder with different Cr3C2 and FeV50 content. The results showed that Fe-based coatings were uniform and dense. The constituent phases were mainly composed of α-Fe solid solution with the increase of Cr3C2 and FeV50, γ-Fe and V8C7 phases were achieved. The microstructure of the coatings exhibited a typical dendrite structure. The concentration of C, V and Cr were saturated in dendritic areas, and the other alloying elements were mainly dissolved in the interdendritic areas. The hardness and wear resistance of Fe-based coatings were enhanced with the Cr3C2 and FeV50 addition. The specimen with 15% Cr3C2 and 16% FeV50 had the highest hardness of 66.1 ± 0.6 HRC, which was 1.05 times higher than the sample with 4.5% Cr3C2 and 5% FeV50, and the wear resistance of the former was three times greater than the latter.