This paper proposes a novel simplified model which describes the real part (in-phase component) of the difference in pickup coil voltage, when an eddy current (EC) sensor consisting of tow coils (excitation and pickup coils) is placed above a titanium (Ti) alloy sheet. A parameter that encapsulates the coil geometry factors is integrated into the classical Dodd-Deeds model, and then the model is simplified by combining with the electromagnetic properties of Ti alloy. The use of the simplified model provides a thickness measurement method for Ti alloy sheets. The measured thickness can be calculated directly from the calibration signal by using the model, without the need to predict response by solving forward model in advance. Experimental measurements were conducted on TC4 (Ti-6Al-4V) Ti alloy sheets of different thicknesses with a developed EC sensor and measurement system. The experiment verified the proposed model and measurement method. The experimental results shown that the maximum measurement error is less than 2.86%, which is greatly lower than the permissible error of the current industry standard. This study provides a theoretical basis and a fast method for EC thickness measurement of Ti alloy.
In the process of eddy current testing (ECT) of surface and subsurface defects of aviation aluminum alloy plates, the setting of parameters is important to the test results. Inappropriate test parameters can cause false detection or even missed detection of defects. To address this problem, the effects of probe type, coil size, and excitation frequency on the accurate identification and quantitative evaluation of surface and subsurface defect detection were studied and analyzed in this study to determine the best testing parameters. The experimental results show that the absolute probe with an outer radius of 3.3 mm has better detection performance for aviation aluminum alloy plate defects. There are different optimal excitation frequency ranges for the surface and subsurface defects. An excitation frequency of 80 kHz to 90 kHz can be used for the detection of unknown defects.