Objective: To compare the fluoride release from Conventional Glass Ionomer Cement (GIC), Resin Modified GIC (RMGIC), and Cention N Alkasite Material. Material and Methods: Forty- five disc-shaped specimens of three different restorative materials (Conventional GIC, RMGIC, and Alkasite material) were made and divided into 3 groups (n=15). Fluoride release was evaluated at the end of Day 1, 7, 14, and Day 28 using fluoride ion-selective electrode. Intergroup and Intra-group analysis was done using One-way ANOVA with a Post-hoc test. A p-value of <0.05 was considered statistically significant. Results: Cention showed more fluoride release (in parts per million) than GIC and RMGIC at increased time duration. However, at the end of day 1, there was lesser fluoride release with Cention, as compared with the other groups. Conclusion: The new Alkasite restorative material showed promising results in terms of fluoride release and is better than GIC and RMGIC at increased time duration.
1 January 2021 in Pesquisa Brasileira em Odontopediatria e Clínica Integrada
The use of resin-based dental composites is multiplying through the years due to the increased demand for tooth-colored restorations. The choice of monomers strongly determines the viscosity, reactivity, mechanical property, water sorption and polymerization shrinkage of the composite material. It is desirable for all monomers to be converted into polymers (Degree of Conversion), but this does not occur clinically, resulting in a poor prognosis for restorations as well as an increase in systemic health risks. The release of monomers occurs due to erosion and degradation, as well as the release of leachable species from the restoration. The potential toxicity of free monomers to dental pulp cells is concerning. Free monomers are not only allergens but also have reported cytotoxic and genotoxic effects. Various methods and practices have thus been employed to counter the ill effects of free monomer release from dental composite restorations for better safety and healthy oral cavities.
In today's era, erosion is the most prevalent type of tooth wear. The prevention of demineralization with biomineralization is the most desired treatment. The aim of this study is to evaluate and compare the surface remineralization potential of two remineralizing agents - self-assembling peptide P11-4 (SAP P11-4) and calcium silicate plus sodium phosphate (CSSP) salts on intact and demineralized enamel using laser-induced breakdown spectroscopy (LIBS). Sixteen maxillary premolars were decoronated and split into buccal and palatal halves embedded in acrylic resin with a total sample size of 32 designated into Group 1 (intact teeth) and Group 2 (demineralized teeth). Further subdivision into Groups 1a and 2a (SAP P11-4 group [n = 8]); Groups 1b and 2b (CSSP group [n = 8]), Group 2 was first exposed to Coca-Cola. Then, all groups were subjected to experimental LIBS. Groups 1a and 2a were treated with SAP P11-4 based product, i.e., CURODONT™ PROTECT gel. Groups 1b and 2b were treated with CSSP-based products regimen, i.e., REGENERATE Enamel Science™ Advanced Toothpaste and Advanced Enamel Serum. The LIBS assessment was redone for all groups to attain a change in Ca and P values. Inferential statistics were done using Wilcoxon signed-rank test (Before-After product application) and Mann-Whitney U-test (between the groups). According to the statistical evaluation there was a statistically significant difference (P < 0.05), in Ca and P values in demineralized teeth when both SAP P11-4 and CSSP groups were evaluated. Although Ca values exhibited a significant difference in intact teeth, P did not exhibit a significant difference on the application of both remineralizing agents. The remineralizing potential between the two agents, SAP P11-4 and CSSP groups. There was no statistically significant difference ( P <0.05) observed between the two agent's remineralization potential for intact and demineralized teeth. SAP P11-4 and CSSP have the potential to remineralize both intact and demineralized enamel. There was increased remineralization in demineralized samples subjected to erosion.
Introduction and Aim: Despite being popular, composite materials frequently degrade, and cause secondary caries in the oral cavity. Studies suggest that surface characteristics, particularly surface roughness, can impact the functionality, durability, and biofilm formation of these materials. This study was carried out to evaluate and compare the surface roughness of nano-ceramic restorative and bulk-fill flowable composite materials and their bacterial adhesion properties using Streptococcus mutans. Materials and Methods: 16 disks of each composite type, Ceram x SphereTEC one universal nano-ceramic restorative material and SDR flow plus bulk-fill flowable material were fabricated and grouped as A and B, respectively. 2D surface roughness of the samples were recorded using Contact Profilometer. For bacterial adhesion test, samples were incubated in a culture of S. mutans overnight. Adhered bacteria were determined by spread plate technique, colonies were enumerated and reported as CFU/mL. Kolmogorov-Smirnov and Shapiro-Wilk tests helped determine normality distribution of surface roughness, and statistical significance was analysed using Independent-samples t test. Bacterial adhesion was analysed using Mann-Whitney U test. Results: Surface roughness values were found to be normally distributed, and the difference between the two groups was noted to be statistically significant (p0.05). Conclusion: Surface roughness value of the nano-ceramic restorative material was lower than that of bulk-fill flowable resin material albeit, the two composites did not show a significant difference in terms of bacterial adherence.
1 January 2021 in Pesquisa Brasileira em Odontopediatria e Clínica Integrada