Lattice-parameter mismatch-induced strains in three-dimensional coherent InxGa1-xAs islands grown on GaAs(001) substrates have been determined experimentally on an atomic scale by a digital analysis of images obtained by high-resolution transmission electron microscopy. The strain distributions in the islands were simulated by finite-element calculations. The simulated strain distributions are found to be in good agreement with measured data, taking into account the thin-foil relaxation of electron-transparent specimens in addition to the well known elastic strain relief. Clear evidence is given for an indium segregation causing a misfit gradient between the interface and the islands' surface.
Efficient resonant excitonic waveguiding is achieved in laser structures, grown by metallorganic chemical vapor deposition, with stacked CdSe quantum islands which were separated by ternary ZnSSe barriers. Plastic relaxation within the stack is shown to be suppressed by adjusting the sulfur content in the barriers to compensate the strain. Excitonic lasing with low threshold intensities is demonstrated well above room temperature with and
The shape transformations and the mechanism of misfit strain relaxation of In0.6Ga0.4As islands grown at different temperatures on GaAs(001) substrates have been investigated. Layers with a constant nominal thickness of 12 monolayers were deposited by molecular beam epitaxy on nominal singular and on vicinal substrates. The specimens were characterized by scanning electron microscopy, transmission electron microscopy and high‐resolution transmission electron microscopy. It is shown that an increase of the growth temperature yields a shape transition from rounded islands to elongated cigar‐like structures. The lattice‐parameter mismatch in the circular islands is relaxed by misfit dislocations at lower growth temperatures. Indium desorption effectively reduces the mismatch at higher growth temperatures and therefore yields the nucleation of coherent islands. In spite of this structural transformation an Arrhenius‐like behaviour of the island densities is observed with an activation energy which depends on the substrate tilt.
Transmission electron microscopy (TEM) and photoluminescence (PL) spectroscopy were applied to study the metalorganic chemical vapor deposition of InGaN and the correlation between the structural properties and luminescence of -quantum well structures. A series of samples was grown varying only the growth duration for the InGaN under otherwise unaltered growth conditions. Composition analyses were carried out by measuring local lattice parameters from TEM images, which are directly related to the local In concentration. A rising average In concentration from 6.5% to 15.4% and a decreasing growth rate are observed with increasing growth duration. All samples show an inhomogeneous In distribution containing In-rich agglomerates with a size of only a few nanometers and less pronounced composition fluctuations on a scale of some 10 nm. The redshift of the PL peak energy with increasing quantum well thickness indicates that the luminescence is predominantly determined by the piezoelectric field.
We investigate the growth of highly strained ultrathin CdS/ZnS quantum well structures by molecular-beam epitaxy with an emphasis on structural aspects such as surface morphology of the growing layer and strain relaxation. As shown by quantitative reflection high-energy electron diffraction (RHEED) measurements, no true three-dimensional nucleation of CdS takes place despite the high mismatch relative to the ZnS buffer. Nevertheless, the CdS surface reveals a high density of very small typically monolayer islands, leading to a strong elastic relaxation at the surface. A new RHEED technique is applied to distinguish this elastic deformation from plastic relaxation through misfit dislocations. The critical thickness for the onset of the latter is found to be three monolayers. This result is confirmed by transmission electron microscopy and photoluminescence measurements carried out for further characterization, proving the presented RHEED technique to be reliable.
Stacking-fault pairs in ZnSe/ZnMgSSe quantum-well structures are found to induce enhanced radiative recombination visible as pairs of bright spots in microphotoluminescence intensity maps. Structural investigation by atomic-force microscopy and transmission electron microscopy (plan view as well as cross section) reveal that a widening and bending of quantum wells occurs when they are intersected by Frank-type stacking faults. The enlargement of the well width by up to 12 bilayers evokes an efficient localization of excitons. The localizing potential related to Shockley-type stacking-fault pairs is found to be much shallower.