4 May 2022 in Scripta Materialia
19 February 2016 in CrystEngComm
We report a magnetically-anisotropic PrCo5 permanent bulk magnet, prepared by a hot deformation method, with crystallographic orientation-dependent magnetic properties. Although the PrCo5 crystals strongly favor the {0001} orientation texture, the crystallographic orientation textures of PrCo5 crystallites differ at various radial locations. From the bulk center to the edge, the c-axis orientation texture decreases from 5.4 MRD to 4.1 MRD, whereas the remanence decreases from 8.93 kGs to 7.58 kGs and the coercivity increases from 4.34 kOe to 6.56 kOe. This paper also reports the alteration of boundary plane orientation textures, resulting from the corresponding energy anisotropy at different locations, and suggests that the development of grain boundaries with lower boundary energies has a significant impact on the magnetic properties with regard to remanence and energy density. The current work therefore proposes an elegant approach to attain desired magnetic properties in PrCo5 magnets by fine-tuning the crystallographic orientation.
27 October 2023 in Journal of Rare Earths
11 August 2020 in IEEE Transactions on Magnetics
The effect of doping Cu on the mechanical properties and magnetic properties of Sm(Co0.71Fe0.15Cu0.07Zr0.03)7.6 magnets was studied systematically. The results show that the Cu-lean grain boundaries and bending strength of the magnet can be improved by increasing of doping Cu content. The optimal magnetic properties of magnet with 1.0 wt.% Cu doping are: Br=9.9 kG, Hcj=23.0 kOe, and (BH)max =22.2 MGOe. With the doping content of Cu powders, the bending strength first reach a peak value of 143.0 MPa at 1.0 wt.% and then drop. The bending strength of the magnet with 1.0 wt.% Cu doping is about 51.8% higher than that of the magnet with 0 wt.% Cu doping. The coercivity and bending strength of the magnet are improved.
30 May 2022 in Materials Research Letters
SmCo7-based permanent magnets with a TbCu7-type structure have excellent high-temperature performance. However, most of the previously reported SmCo7 nanocrystalline magnets were isotropic, which limited their application. So the preparation of anisotropic SmCo7 magnets with preferred texture is still a challenge. In this work, we prepared anisotropic SmCo6.8Hf0.2 nanocrystalline magnets by hot pressing and hot deformation method. EBSD results indicated that the {0001} orientation texture of the hot deformed magnet was remarkably preferred, which further improved the remanence. Subsequently, the structural evolution process was systematically characterized by TEM. It provides crucial insight for developing high-performance SmCo7-based magnets. Impact Statement: Up to now, most of the previously reported SmCo7 nanocrystalline magnets were isotropic, which limited their application. This work opens up new opportunities to create high-performance SmCo7-based nanostructured magnets. GRAPHICAL ABSTRACT