Perovskite oxides with mixed ionic and electronic conductivities are very promising candidates for their application as energy materials related to fuel cell and metal air battery integration. In this article, we report on the systematic characterization of mixed proton and electron conducting compounds of composition BaFe1−xCoxO3−y−δ(OH)y synthesized via nebulized spray pyrolysis. Independent of the value of x, all samples BaFe1−xCoxO3−y−δ(OH)y were found to crystallize in an orthorhombic ordering/distortion variant of the perovskite type structure (space group Cmcm) and are isotypic to the border phases (x = 0 or 1) reported previously. A minimum water content was observed for the composition with x = 0.5, which increases steadily for Co or Fe richer compositions. Impedance studies show that the conductivity increases with increasing Co-content, with BaCo0.5Fe0.5O2.07(OH)0.74 showing a total electrical conductivity of 10−7 S cm−1 at 298 K, an order of magnitude higher than found for BaFeO2.33(OH)0.33. Further, bifunctional catalytic activity for the oxygen evolution reaction (OER) and oxygen reduction reaction (ORR) was found for the compounds of the series as investigated in 0.1 M KOH, with BaFe0.8Co0.2O3−y−δ(OH)y possessing the best bifunctional performance parameter of ΔU = 1.10 V, which is comparable to that of other non-precious metal catalysts.
In the present work, monolithic SiC/(Hf0.75Ta0.25)C(N)/(B)C ceramic composites are prepared via spark plasma sintering of amorphous SiHfTa(B)CN‐based powders synthesized from single‐source precursors. The as‐sintered ceramic nanocomposites are investigated by X‐ray diffraction, Raman, scanning electron microscopy, and transmission electron microscopy in order to study their microstructure and chemical composition. Furthermore, the thermal conductivity, the thermal expansion, as well as the hardness and Young's moduli of the prepared monolithic samples are determined. The incorporation of boron in the system results in enhanced densification due to decreased porosity and improved distribution of the individual phases in the composite after sintering. These favorable effects also positively influence the thermomechanical properties of the composite. The boron‐modified sample displays a decreased thermal diffusivity and conductivity compared with the boron‐free sample. Additionally, a macro‐hardness obtained by Vickers indentation of 31 GPa is achieved for loads up to 196 N, surpassing the hardness of ultrahard materials like silicon carbide, hafnium carbide, and tantalum carbide as well as their solid solutions. Young's moduli of the composites were analyzed to 405 ± 10 and 277.5 ± 41 GPa for the boron‐containing and boron‐free samples, respectively.