Eveline Nicole Reinheimer

Eveline Nicole Reinheimer

Auto-generated profile, based on publicly available information

Eveline Nicole Reinheimer

IFSW, University of Stuttgart, Stuttgart, Germany

Research Focus & Metrics

Academic Career Length

7Years (2020-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
21 June 2022 in European Journal of Mechanics - B/Fluids
Verified
Journal Article
Closed access
DSDaniel Sollich
Daniel Sollich
EREveline-Nicole Reinheimer
Eveline-Nicole Reinheimer
JWJonas Wagner
Jonas Wagner
PBPeter Berger
Peter Berger
PEPeter Eberhard
Peter Eberhard

13 July 2023 in Journal of Laser Applications
Verified
Journal Article
Open access
PDF file
MOMarkus Omlor
Markus Omlor
EREveline Nicole Reinheimer
Eveline Nicole Reinheimer
TBTom Butzmann
Tom Butzmann
KDKlaus Dilger
Klaus Dilger
Electric drives continue to grow in importance for future mobility. In recent years, hairpin winding has become established for stator production. For connecting rectangular hairpin ends, a laser beam welding process is usually implemented. For sufficient vibration resistance and current carrying capacity, pores must be avoided. This work investigates the pore formation by using a high-speed x-ray imaging system during the welding process of hairpins. This allows us to observe the formation of pores during the welding process using x-ray videos. Specifically, the use of different intensity distributions with static beam shaping (ring and core shape) is analyzed. In addition, the welding speed and the use of a protective gas (argon and helium) are taken into account. The welding results are evaluated with an x-ray CT-analysis. It is found that the formation of pores most likely occurs at the transition area of one pin end to the other. The results also show that with different intensity profiles of the laser beam, the number of process pores occurred can be influenced and reduced. An optimum welding speed and the use of a protective gas also have positive effects on pore formation.

14 June 2022 in Journal of Laser Applications
Verified
Journal Article
Open access
PDF file
EREveline N. Reinheimer
Eveline N. Reinheimer
RWRudolf Weber
Rudolf Weber
TGThomas Graf
Thomas Graf
High-speed laser welding is a very efficient process that results in weld seams of high quality. The process is limited by the occurrence of weld defects, such as humping and undercuts. It was found that a transition from a weld without defects to a weld with undercuts occurs when a speed limit is exceeded. It was also found that undercuts occur at slightly lower feed rates than humping. Thus, it was concluded that undercuts represent the upper process limit of high-speed laser welding and may be seen as the precursor of the humping regime.

23 February 2024 in The International Journal of Advanced Manufacturing Technology
Verified
Journal Article
Open access
PDF file
EREveline N. Reinheimer
Eveline N. Reinheimer
PBPeter Berger
Peter Berger
CHChristian Hagenlocher
Christian Hagenlocher
RWRudolf Weber
Rudolf Weber
TGThomas Graf
Thomas Graf
The advent of undercuts and humping limits the applicable speed of deep-penetration laser welding. Recent findings additionally show that a significant change of the keyhole’s shape is associated with the occurrence of undercuts. Considering that undercuts and humping are melt flow–induced defects, this leads to the question of how the geometry of the keyhole and the melt pool influence the melt flow and vice versa. In this work, the Froude number was used to characterize the melt flow around a keyhole. X-ray images of the keyhole and cross-sections of the weld were therefore used to determine the geometrical boundaries of the melt flow, to estimate the average melt velocity around the keyhole, and finally determine its Froude number. The flow around a cylindrically shaped keyhole was found to always be subcritical, whereas supercritical melt flow was observed around the elongated keyholes that are formed at higher welding speed. The findings may be interpreted in the sense that the elongation of the keyhole is a consequence of a supercritical stream of the melt flowing underneath and around the keyhole. This perception is consistent with the long-known experience that humping may be avoided by reducing the flow speed of the melt by widening the melt pool surrounding the keyhole (e.g., by means of beam shaping) and suggest a new explanation for the elongation of the keyhole at increased welding speed.

27 February 2025 in The International Journal of Advanced Manufacturing Technology
Verified
Journal Article
Open access
PDF file
EREveline Nicole Reinheimer
Eveline Nicole Reinheimer
MHMichael Haas
Michael Haas
FZFelix Zaiß
Felix Zaiß
MOMarkus Omlor
Markus Omlor
CSChristoph Spurk
Christoph Spurk
TGThomas Graf
Thomas Graf
Any pores formed during laser welding of copper hairpins affect the structural integrity and the mechanical/electrical functionality of the joint. We report on investigations using synchrotron X-ray imaging techniques to observe the formation of the pores in the processing zone while welding. It was found that all pores are formed at the joint gap and that the small pores are distributed throughout the complete joint volume as a result of the melt flow induced by the movement of the laser beam. This insight has led to the development of a welding strategy that minimizes pore formation by avoiding the movement of the laser beam across the joint gap. This was achieved by rapid beam shaping based on coherent beam combining (CBC) technology.

1 May 2020 in Journal of Laser Applications
Verified
Journal Article
Closed access
PDF file
EREveline N. Reinheimer
Eveline N. Reinheimer
EWErnst Wolf
Ernst Wolf
RWRudolf Weber
Rudolf Weber
TGThomas Graf
Thomas Graf
Aging, growth of whisker, and thermal damage are the major issues when soldering electronic components. The authors present investigations to determine the influence of process times on the threshold temperature leading to thermal damage in epoxy-based printed circuit boards (PCBs). Experimentally verified numerical modeling was used to determine the temperature distribution at the interface of copper and the epoxy resin. The results show that the threshold temperature significantly increases with decreasing process times. With interaction times shorter than 5 ms, the threshold temperatures are found to be 900 K higher than the ones specified for longer heating times according to the data sheet for PCBs with FR4 epoxy resin.