Electrochemical production of acid and base from water enables their use as regenerable reagents in closed-loop processes, with attractive applications including CO2 capture or mineralization and low-temperature production of Ca(OH)2. Conventional systems utilize ion exchange membranes (IEMs) to inhibit H+/OH– recombination, which leads to high resistive losses that compromise energy efficiency and poor tolerance for polyvalent metal ions that complicates applications involving mineral resources. Here we use ion transport modeling to guide the design of a system that uses a simple porous separator instead of IEMs. Using H2 redox reactions for H+/OH– production, we demonstrate acid-base production at useful concentrations in the presence of polyvalent impurities with lower energy demand and higher current density than reported IEM-based systems. Cells can be stacked by combining H2 electrodes into a bipolar gas diffusion electrode, which recirculates H2 with near-unity efficiency. We show that the cell outputs extract alkalinity from olivine and serpentine as Mg(OH)2 and Mg3Si2O6(OH)2, which remove CO2 from ambient air to form Mg carbonates. These studies establish the principles for membrane-free electrochemical acid-base production, enabling closed-loop resource recovery and material processing powered by renewable electricity.
Rapidly growing demand for lithium-ion batteries (LIBs) necessitates a significant expansion of LIB recycling to ensure adequate supply and avoid waste buildup. Traditional hydrometallurgical LIB recycling processes use super-stoichiometric quantities of acid and base and generate large volumes of salt waste that pose an environmental burden. Electrochemical regeneration of acid and base from salt offers a zero-waste alternative but faces challenges with respect to throughput and energy consumption, with current densities typically limited to ≤ 100 mA/cm2 and energy demands > 0.10 kWh/mol. These limitations stem from a reliance on ion exchange membranes (IEMs), which lead to high cell resistance. This study reports a hydrometallurgical process to recycle lithium cobalt oxide (LCO) and lithium nickel manganese cobalt oxide (NMC) cathodes using acid and base electrochemically generated from a Li2SO4 electrolyte. The electrochemical cell used contains no IEMs, enabling excellent energy efficiency between 0.033 and 0.097 kWh/mol at current densities up to 500 mA/cm2 and imparting a robust tolerance for impurities that typically foul IEMs. The produced acid and base are found to be competent for etching and recovering > 90% of the valuable metals from LIBs at industrially relevant pulp densities up to 66 g/L and are readily regenerated from the salt solution left at the end of the metal recovery process.
The dramatic expansion of Li-ion batteries (LIBs) today necessitates a similar expansion of LIB recycling to recover the critical mineral content of > 500 GWh worth of spent batteries and scrap anticipated as soon as 2030. The dominant hydrometallurgical route for recycling LIBs uses strong acid and base to leach and recover the valuable metals from battery cathodes. However, the process suffers from a significant salt waste burden, with 1.5 tons of impure Na2SO4 salt waste generated per ton of cathode material. This waste stream may instead be used to regenerate strong acid and base for hydrometallurgical recycling, creating a circular process and avoiding the need for continuous input of acid and base. Electrochemical systems for generating acid and base from such streams reported thus far operate at low current densities (<100 mA/cm2) and have a high energy demand, preventing their adoption at scale.
Rapidly growing demand for lithium-ion batteries (LIBs) necessitates a significant expansion of LIB recycling to ensure adequate supply and reduce environmental burdens. Traditional hydrometallurgical LIB recycling processes use superstoichiometric quantities of acid and base and generate large volumes of salt waste. Electrochemical regeneration of acid and base from salt offers a zero-waste alternative but faces challenges with respect to throughput and energy consumption. This study reports a hydrometallurgical process to recycle lithium cobalt oxide (LCO) and lithium nickel manganese cobalt oxide (NMC) cathodes using acid and base electrochemically generated from a Li2SO4 electrolyte. The electrochemical cell used contains no ion exchange membranes, enabling excellent energy efficiency between 0.033 - 0.097 kWh/mol at current densities up to 500 mA/cm2 and imparting a robust tolerance for impurities that typically foul IEMs. The produced acid and base are found to be competent for etching and recovering >90% of the valuable metals from LIBs at industrially relevant pulp densities up to 66 g/L, and are readily regenerated from the salt solution left at the end of the metal recovery process.
21 October 2026 in Journal of the American Chemical Society
Rapidly growing demand for lithium-ion batteries (LIBs) necessitates a significant expansion of LIB recycling to ensure adequate supply and avoid waste buildup. Traditional hydrometallurgical LIB recycling processes use super-stoichiometric quantities of acid and base and generate large volumes of salt waste which pose an environmental burden. Electrochemical regeneration of acid and base from salt offers a zero-waste alternative but faces challenges with respect to throughput and energy consumption, with current densities typically limited to ≤ 100 mA/cm 2 and energy demands > 0.10 kWh/mol. These limitations stem from a reliance on ion exchange membranes (IEMs), which lead to high cell resistance. This study reports a hydrometallurgical process to recycle lithium cobalt oxide (LCO) and lithium nickel manganese cobalt oxide (NMC) cathodes using acid and base electrochemically generated from a Li 2 SO 4 electrolyte. The electrochemical cell used contains no IEMs, enabling excellent energy efficiency between 0.033 - 0.097 kWh/mol at current densities up to 500 mA/cm 2 and imparting a robust tolerance for impurities that typically foul IEMs. The produced acid and base are found to be competent for etching and recovering > 90% of the valuable metals from LIBs at industrially relevant pulp densities up to 66 g/L, and are readily regenerated from the salt solution left at the end of the metal recovery process.