Rutile-phase TiO2 films were epitaxially grown on Si(100) substrates by oxidizing epitaxial TiN films grown by KrF pulsed excimer laser deposition. The TiO2 film was (110)-oriented and composed of two domains perpendicular to each other in the plane. The electrical resistivity at 2.5 V and the dielectric constant at 1 MHz of the film were 1.1×1010 Ω· cm and 49, respectively. This film could be used as a buffer layer for the growth of epitaxial BaTiO3 film on Si. The BaTiO3 (260 nm)/TiO2 (230 nm) double-layered film showed a high dielectric constant (ε r=91) and a very low leakage current of 5×10-8 A/cm2 at 10 V.
NiO nanowires were formed along atomic step edges on the ultrasmooth sapphire (0001) substrates by laser molecular beam epitaxy. From atomic force microscopy, the nanowires were found to be ∼20 nm in width and ∼0.5 nm in height along the straight, 0.2 nm-high step edges of the substrate. The crystal structure of NiO nanowires was examined by in situ coaxial impact collision ion scattering spectroscopy (CAICISS). The CAICISS results on the azimuth dependences of Ni signal for the NiO nanowires as well as NiO (111) epitaxial thin films indicate that the NiO nanowires were epitaxially grown with (111) orientation under in-plane stress.
1 September 2020 in Nuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms