We have investigated the structural, optical band gap, and electrical properties of (Fe2O3)0.5x:(NiO)1 − 0.5x (x = 0.3, 0.4, 0.5, 0.6 and 0.7) epitaxial thin films grown on an atomically smooth substrate at room temperature. With increasing Fe2O3 content, the rock-salt structure of the thin films transformed to a spinel structure above x = 0.6. In terms of the local structure, the increased ratio of Fe2+ ions to Fe3+ ions indicates that the octahedral sites of FeO were continuously transformed into distorted octahedral and tetrahedral sites. On the other hand, the NiO matrix was not affected by the local structure change. Chemical composition of Fe2O3:NiO affected the crystal structure, the electrical conductivity and the optical band gap of direct transition (3.35 to 2.99 eV).
Thin-film epitaxy is critical for investigating the original properties of materials. To obtain epitaxial films, careful consideration of the external conditions, i.e. single-crystal substrate, temperature, deposition pressure and fabrication method, is significantly important. In particular, selection of the single-crystal substrate is the first step towards fabrication of a high-quality film. Sapphire (single-crystalline α-Al2O3) is commonly used in industry as a thin-film crystal-growth substrate and functional thin-film materials deposited on sapphire substrates have found industrial applications. However, while sapphire is a single crystal, two types of atomic planes exist in accordance with step height. Here we discuss the need to consider the lattice mismatch for each of the sapphire atomic layers. Furthermore, through cross-sectional transmission electron microscopy analysis, we demonstrate the uniepitaxial growth of cubic crystalline thin films on bistepped sapphire (0001) substrates.
1 January 2005 in Japanese Journal of Applied Physics
NiO nanowires were formed along atomic step edges on the ultrasmooth sapphire (0001) substrates by laser molecular beam epitaxy. From atomic force microscopy, the nanowires were found to be ∼20 nm in width and ∼0.5 nm in height along the straight, 0.2 nm-high step edges of the substrate. The crystal structure of NiO nanowires was examined by in situ coaxial impact collision ion scattering spectroscopy (CAICISS). The CAICISS results on the azimuth dependences of Ni signal for the NiO nanowires as well as NiO (111) epitaxial thin films indicate that the NiO nanowires were epitaxially grown with (111) orientation under in-plane stress.