Amol Thakare

Amol Thakare

Auto-generated profile, based on publicly available information

Amol Thakare


Research Focus & Metrics

Academic Career Length

1Year (2026-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
18 May 2026 in SSRN Electronic Journal
Verified
Preprint
Open access
LSLarissa Juliana Sirtuli
Larissa Juliana Sirtuli
ATAmol Thakare
Amol Thakare
SNSusanne Norgren
Susanne Norgren
JÖJonas Östby
Jonas Östby
SSSiamak Shoja
Siamak Shoja
CVD α-Al2O3 coatings on cemented carbides are widely used in steel turning, where cutting tool performance is strongly dependent on the crystallographic texture of the α-Al2O3 layer. Residual stress, cooling-crack density, and hardness are key factors influencing coating integrity during machining. Although texture has been reported to affect these properties, trends remain inconsistent in the literature. In this work, three CVD α-Al2O3/Ti(C,N) coatings with identical architecture, substrate, and processing route, but distinct α-Al2O3 textures: i. c-plane (0001) , ii. r-plane (01-12) , and iii. a-plane (11-20) were investigated to isolate the role of texture under controlled conditions. The (0001) coating exhibited the highest tensile residual stress and the lowest crack density, while the (01-12) and (11-20) coatings showed lower stresses and denser crack network. This behaviour is consistent with a texture-dependent thermal expansion mismatch, complemented by orientation-dependent stress accommodation during cooling. The (01-12) and (11-20) textures, with a greater in-plane contribution of the c-axis, develop higher intrinsic thermal stress and thus promote more extensive crack formation for stress relaxation compared to texture. Nanohardness values were comparable across the three textures. The results demonstrate that α-Al2O3 texture has a clear influence on residual stress and cracking, but a limited effect on hardness. These findings provide a more consistent basis for interpreting texture–property relationships and suggest that the performance of (0001)-textured coatings in steel turning is primarily associated with reduced crack density and their response under directional loading, rather than with differences in hardness.

21 February 2026 in SSRN Electronic Journal
Verified
Preprint
Open access
ATAmol Thakare
Amol Thakare
JFJonas Faleskog
Jonas Faleskog
FLFredrik Lindberg
Fredrik Lindberg
LTLisa Toller-Nordström
Lisa Toller-Nordström
JÖJonas Östby
Jonas Östby
A TiCN–αAl2O3 bilayer coating on a WC–Co substrate is studied to investigate if inelastic strains arise from the chemical vapor deposition process. Both as-deposited and blasted coatings are studied. Due to a mismatch in the coefficients of thermal expansion, tensile residual stresses arise in the coating layers during cooling down to room temperature after deposition, which leads to nucleation of surface cracks. The residual stresses remaining in the coating layers are estimated from X-Ray Diffraction measurements. Nanoindentation is used to determine a hardness value for each coating layer which is adjusted for size effects and then transformed to a representative flow stress using Tabor’s formula. The representative flow stress is found to be an order of magnitude larger than the residual stresses in the coatings, indicating that inelastic deformation during application can be ruled out. SEM-EBSD is used to characterize cross-sections of both as-deposited and blasted coatings. The EBSD maps show no sign of inelastic deformation in the as-deposited coatings, whereas in blasted coatings, only the top layer of Al2O3 show clear evidence of inelastic strains.