1 June 2018 in Surface and Coatings Technology
1 March 2019 in Surface and Coatings Technology
1 April 2018 in Surface Engineering
The iron-containing layers were produced on the 2024 alloy surface using ultrasonic impact treatment (UIT) in the ambient air and argon environment. Multiple high-energy collisions of the pin of Armco-iron by the treated surface induce the iron cladding by means of solid-state welding of Fe dopants and Al substrate. SEM and EDX analysis and microhardness measurements showed a formation of oxide/intermetallic layers, which thickness ranges from 15–20 to 30–35 μm and hardness achieves ∼4 and ∼9 GPa after the argon-UIT and air-UIT processes, respectively. The polarisation tests in 3.5%NaCl medium showed that the layers are characterised by lower corrosion rates and more positive corrosion potentials than those of the original alloy owing to the formation of Alx-Fey intermetallics. The noblest behaviour was registered for the air-UIT-processed 2024 alloy.
1 February 2013 in Applied Surface Science
28 October 2013 in Journal of Applied Physics
FePt thin films with a thickness of 30 nm were deposited by dc magnetron sputtering at room temperature onto SiO2(100 nm)/Si(100) substrates. These films were post-annealed in a temperature range of 500 °C to 900 °C for 30 s in three different atmospheres—N2, Ar, and forming gas (Ar+H2 (3 vol. %)). Irrespective of the annealing atmosphere, the chemically ordered L10 FePt phase has formed after annealing at 500 °C. Higher annealing temperatures in N2 or Ar atmosphere resulted in a strong increase in grain size and surface roughness but also in the appearance of a pronounced (001) texture in the FePt films. However, these films show the presence of iron oxide. In contrast, annealing in forming gas atmosphere suppressed the oxidation process and resulted in a reduced grain size and lower surface roughness. However, no (001)—but a strong (111)—texture was obtained after annealing at 700 °C, which might be related to the reduced unit cell tetragonality and incorporation of hydrogen to the FePt lattice. Thus, this study clearly demonstrates that the oxygen/hydrogen content plays an important role in controlling the crystallographic orientation during post-annealing.
7 September 2013 in Applied Physics A