This study examined the microstructure characteristics, electrical resistivity (ER), and mechanical properties of ultra-high-performance concrete (UHPC) made with nano-silica (NS), electric arc furnace slag (EAFS), and waste glass powder (WGP). Eight concrete mixtures of binary and ternary blends were assessed to investigate the possible relationships between the observed physical and microstructural features with the obtained compressive and flexural strengths. The individual and combined effects of NS, EAFS (up to 50% replacement of silica sand), and WGP (up to 30% cement replacement) on the examined properties were evaluated. Scanning electron microscopy (SEM), thermogravimetric (TG) analysis, X-ray diffraction (XRD), ER, and pH values, and measurements were employed. SEM examination indicated that using NS along with EAFS and WGP reduced gap space around the fiber, and the enormous single cracks turned into numerous small cracks, thereby improving bonding and flexural strength. TG and XRD studies supported this finding. The ER for the EAFS specimens was enhanced without compromising the alkalinity range of concrete, as proved by pH tests, which address the possible corrosion problem of reinforcement. Thus, sustainable UHPC is achievable.
30 December 2023 in Engineering and Technology Journal
Quartz powder is used in ultra-high-performance concrete to improve granular packing, but repeated inhalation during manufacture can cause health issues. The mechanical properties of UHPC are influenced by the post-setting curing method. A hypothesis suggests limestone powder could be a viable filler to mitigate these issues under three different curing regimes, replacing quartz powder of similar size. The study assessed 18 mixtures with different w/b ratios for flow characteristics and compressive strength after 7 and 28 days of curing under various conditions. Limestone powder positively impacted compressive strength and had fresh properties. A two-factor interaction model accurately correlated variables and responses. Numerical optimization was performed to find the optimal mixture with proper flow and the highest compressive strength. The use of 150 kg/m3 of locally sourced limestone powder in the mixture with a w/b ratio equal to 0.198 and a 48hr-90°C curing regime can be considered the optimal amount to secure the greatest modeling compressive strength (169.10 MPa at 7 days and 181.71 MPa at 28 days), fulfilling the limit values of spread flow (220 mm) with the increasing percentage ratio of 67% and 49% at 7-days and 28-days ages under 90°C heat curing when the w/b equals 0.198.
14 February 2025 in European Journal of Environmental and Civil Engineering