Xi’an Structure Function Materials International Science and technology Cooperation Base, School of Materials and Chemical Engineering, Xi’an Technological University, Xi’an, China
Auto-generated profile, based on publicly available information
Pinyang Fang
Xi’an Structure Function Materials International Science and technology Cooperation Base, School of Materials and Chemical Engineering, Xi’an Technological University, Xi’an, China
Ferroelectric ceramics (SBLNO) were prepared by a solid state reaction process. X-ray diffraction analysis indicated that single phase layered perovskites were obtained. The maximum dielectric permittivity peak broadened gradually with the lanthanum content increasing indicated that the phase transition from normal ferroelectrics to relaxorlike ferroelectrics occurs in SBLNO. The modified Curie–Weiss (CW) law was used to describe the relaxor behavior of SBLNO ceramics. The relaxation indication coefficient was estimated from a quadratic fit of modified CW law and was found to be 1.71 and 1.72 for SBLN20 and SBLN30 specimens, respectively. The substitution of ions for ions in the layers resulted in a shift in the Curie point to lower temperature and an increase in remanent polarization and electrical field-induced strain. The maximum strain for SBLN30 specimen was found to be about at the 5 MV/m. The nature of relaxor behavior of SBLNO is attributed to the cationic disordering at nanoscale on site by the substituted of layers.
1 July 2021 in Journal of the American Ceramic Society
A single crystal with nominal composition Pb(Mg1/3Nb2/3)O3-32PbTiO3 (PMN-32PT) was grown by the Bridgman technique. Crystal orientation was determined using the rotating orientation X-ray diffraction (RO-XRD). Element distribution was measured along different directions using inductively coupled plasma-mass spectrometry (ICP-MS). The effect of the element segregation along axial and radial directions on the electrical properties of the PMN-32PT crystal was investigated. It is indicated that the electrical properties of the samples along the axial direction were strongly dependent on the PT (PbTiO3) content. With the increase of the PT content, the piezoelectric coefficient and remnant polarization were improved. Differently, the electrical properties of the samples along the radial direction were mainly determined by the ratio of the Nb and Mg. The reasons for the element segregation and electrical properties varied with the composition were discussed.