Highly uniform electrodeposited Cu2O electrodes for Li-ion batteries, with variable particle size, morphology and thickness, have been studied in the charged and discharged steps as a function of the number of cycling processes, by means of ex situ X-ray absorption spectroscopy (XAS) at the Cu K edge. Both, fingerprint analysis of the X-ray Absorption Near Edge Structure spectra (XANES) and the radial atomic distribution obtained by the analysis of the Extended X-ray Absorption Fine Structure (EXAFS) spectra, have allowed us to quantify the bimodal distribution (Cu and Cu2O) of the electrodes. These results correlate qualitatively well with their different electrochemical response, establishing a deep insight into the reversible reactivity mechanism of these films towards lithium in Li batteries. Our results demonstrate that the reversibility of the reduction process upon the number of cycles depends on the thickness, as it was suggested in previous works but also on the morphology of the electrodes. Higher reversibility corresponds to smaller thickness electrodes. For similar thickness, the reversibility is higher for porous and nanometric particle electrodes than for compact and micrometric particle electrodes. The thinnest film exhibited an increase of capacity after several recycling steps, which agrees with the increase of the Cu2O content.
Deviations of the Sedov-Taylor scaling at three different laser ablation regimes (500 mJ in a 0.8 mm spot, 50 mJ in a 0.8 mm spot and 500 mJ in a 2.5 mm spot) were investigated using Schlieren photography in combination with optical scattering and optical emission spectrometry, among others. For each case, the time evolution of the shock front was related to the formation, expansion and properties of the plasma. Both, the time scale of the different radiative processes and that observed for vapor condensation into nanoparticles and sub-micron particles are compatible with the divergences found between the model and experimental data.